Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
PolyOne Bergamid™ B650 G/Mi20 UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
PolyOne Bergamid™ B700 UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
PolyOne Bergamid™ B700 X2 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Surface Resistance | >= 1.00e+10 ohm | >= 1.00e+10 ohm | DIN 53 482 |
Perstorp Compounds AMITEC VXO UF/MF blend A special Urea Formaldehyde/Melamine Formaldehyde blend that enhances surface properties and is optimized for cost-effective injection molding of visible components.Information provided by Perstorp .. |
|||
Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 2.51e+15 ohm Grade Count:4 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Surface Resistance | 1.00e+10 - 1.00e+13 ohm | 1.00e+10 - 1.00e+13 ohm | Average value: 5.81e+12 ohm Grade Count:7 |
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
Hexion Bakelite™ X24 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled.Application areas: Operating controls, housing parts, lamp holders.Information provided by Bak AGBak AG became a part of Hexion in 2005. |
|||
Surface Resistance | <= 1.00e+10 ohm | <= 1.00e+10 ohm | |
Lehmann & Voss LUVOCOM® TPI-0953 Thermoplastic polyimide, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.Very high continuous use and heat dist.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, Conditioned Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistance.Available in: Asia Pacific, Europe and Latin AmericaProdu.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
Solvay TECHNYL® C 402 M PA6, Conditioned Description: Unreinforced polyamide PA6, high viscosity, containing monomer, for extrusion.Available in: Europe and North AmericaProduct Applications: It is suitable for applications requiring high .. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | DIN 53482 |
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Conditioned Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY KX01002 Acetal Copolymer (Europe-Africa-Middle East) LNP* Stat-Loy* KX01002 is a compound based on Acetal Copolymer resin containing Antistat. Added features include: Permanent Anti-Static. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6000 GS 20 HWCP 20% Glass Sphere Filled Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6000 GS 50 HWCP 50% Glass Sphere Filled Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6000/58 GV 15 HWUVCP 15% Glass Fiber Nylon 6, Impact Modified Until -40°C, UV Stabilized, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
EMS-Grivory Grivory® TSGZ-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
EMS-Grivory Grivory® XE 4188 black 9992 PA612 Product description: Grilamid XE 4188 black 9992 is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 black 9992 are: High v.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6000 GS 50 HWUVCP 50% Glass Sphere Filled Nylon 6, UV Stabilized Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Conditioned, 40% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | |
BASF Novolen® 3248 TC Polypropylene Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IS 3396-1979 |
Amity Thermosets ATI 172 Phenolic Molding Organic and inorganic Filler, Injection Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackVery soft flow .. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
BASF Ultramid® A3WG6 BK 00564 30% Glass Filled PA66 (Conditioned) Description: 30% glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of high stiffness and dimensional stability such as lamp socket housings, f.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Conditioned) Description: 25% mineral-filled and 15% glass-fiber reinforced injection-molding grade for industrial articles having medium rigidity and high dimensional stability, used e.g. for covers and handles.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group MELOPLAS® 180 MF Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing .. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | |
BASF Novolen® 1148 UC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |