| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced |
| Manufacturer | BASF |
| Trade Name | Ultramid® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Conditioned).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
| Water Absorption | 6.3 - 6.9 % | 6.3 - 6.9 % | Saturation; ISO 62 |
| Moisture Absorption at Equilibrium | 1.8 - 2.2 % | 1.8 - 2.2 % | 23°C; 50% RH; ISO 62 |
| Viscosity Measurement | 135 | 135 | ISO 307 |
| Linear Mold Shrinkage | 0.0040 cm/cm | 0.0040 in/in | restricted |
| Melt Flow | 59.2 g/10 min <br>@Load 5.00 kg,<br> Temperature 275 °C |
59.2 g/10 min <br>@Load 11.0 lb,<br> Temperature 527 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527-1/-2 |
| Elongation at Yield | 7.5 % | 7.5 % | 50 mm/min; ISO 527-1/-2 |
| Modulus of Elasticity | 4.30 GPa | 624 ksi | ISO 527-1/-2 |
| Flexural Strength | 120 MPa | 17400 psi | at max force; ISO 178 |
| Izod Impact, Notched (ISO) | 13.0 kJ/m² <br>@Temperature 23.0 °C |
6.19 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 180/A |
| Charpy Impact Unnotched | 7.00 J/cm² <br>@Temperature 23.0 °C |
33.3 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 179/1eU |
| Charpy Impact, Notched | 0.800 J/cm² <br>@Temperature 23.0 °C |
3.81 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 179/1eA |
| Tensile Creep Modulus, 1000 hours | 1850 MPa <br>@Strain <=0.500 % |
268000 psi <br>@Strain <=0.500 % |
ISO 899-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | |
| Thermal Conductivity | 0.380 W/m-K | 2.64 BTU-in/hr-ft²-°F | DIN 52612 |
| Melting Point | 220 °C | 428 °F | DIN 53765 |
| Maximum Service Temperature, Air | 180 °C | 356 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
| Dielectric Constant | 6.2 <br>@Frequency 1.00 Hz |
6.2 <br>@Frequency 1.00 Hz |
IEC 60250 |
| Dissipation Factor | 0.20 <br>@Frequency 1.00e+6 Hz |
0.20 <br>@Frequency 1.00e+6 Hz |
IEC 60250 |
| Comparative Tracking Index | 400 V | 400 V | Test solution A; IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 270 - 290 °C | 518 - 554 °F | Injection-molding/Extrusion |
| Mold Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection-molding |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | BK 30564 | |
| Commercial Status | Europe |