Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+12 - 1.00e+13 ohm | 1.00e+12 - 1.00e+13 ohm | IEC 60093 |
Raschig Group AMPLA® 2000 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+13 ohm | 1.00e+12 - 1.00e+13 ohm | IEC 60093 |
Raschig Group AMPLA® 2500 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+13 ohm | 1.00e+12 - 1.00e+13 ohm | IEC 60093 |
Raschig Group RALUPOL® 4566 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+13 ohm | 1.00e+12 - 1.00e+13 ohm | IEC 60093 |
Raschig Group RALUPOL® 4802 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Surface Resistance | 50.0 - 1.00e+13 ohm | 50.0 - 1.00e+13 ohm | Average value: 1.56e+11 ohm Grade Count:81 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Surface Resistance | 48.0 - 1.00e+13 ohm | 48.0 - 1.00e+13 ohm | Average value: 7.69e+11 ohm Grade Count:11 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+13 ohm | 1.00e+12 - 1.00e+13 ohm | IEC 60093 |
Raschig Group RALUPOL® 802 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+13 ohm | 1.00e+12 - 1.00e+13 ohm | IEC 60093 |
Raschig Group RALUPOL® 804 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+13 ohm | 1.00e+12 - 1.00e+13 ohm | IEC 60093 |
Raschig Group RALUPOL® 8601 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+13 ohm | 1.00e+12 - 1.00e+13 ohm | IEC 60093 |
Raschig Group RALUPOL® 8602 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+13 ohm | 1.00e+9 - 1.00e+13 ohm | ASTM D257 |
PolyOne Edgetek® AS-1000 SD Unreinforced ABS - Antistatic Protection
(discontinued **) Data provided by PolyOne. |
|||
Surface Resistance | 1.00e+9 - 1.00e+13 ohm | 1.00e+9 - 1.00e+13 ohm | ASTM D257 |
PolyOne Stat-Tech™ AS-15GF/000 SD ABS - 15% Glass Fiber Reinforced - Antistatic Protection
(discontinued **)& Data provided by PolyOne. |
|||
Surface Resistance | 1.00e+10 - 1.00e+13 ohm | 1.00e+10 - 1.00e+13 ohm | Average value: 8.42e+12 ohm Grade Count:6 |
Overview of materials for Polyamide-Imide, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+13 ohm | 1.00e+10 - 1.00e+13 ohm | Average value: 5.81e+12 ohm Grade Count:7 |
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+13 ohm | 1.00e+12 - 1.00e+13 ohm | Average value: 7.00e+12 ohm Grade Count:3 |
Overview of materials for Nylon 66, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Surface Resistance | 1.00 - 1.00e+13 ohm | 1.00 - 1.00e+13 ohm | Average value: 2.00e+11 ohm Grade Count:40 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+13 ohm | 1.00e+12 - 1.00e+13 ohm | Average value: 7.00e+12 ohm Grade Count:3 |
Overview of materials for Nylon 66, Mineral Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+13 ohm | 1.00e+12 - 1.00e+13 ohm | Average value: 5.50e+12 ohm Grade Count:4 |
Overview of materials for Nylon 12, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Surface Resistance | 1.00e+11 - 1.00e+13 ohm | 1.00e+11 - 1.00e+13 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY W3000XXJ PBT LNP* STAT-LOY* W3000XXJ is a compound based on PBT. Added features of this grade include: Anti-Stat, Colorable, Healthcare |
|||
Surface Resistance | 1.00e+12 - 1.00e+13 ohm | 1.00e+12 - 1.00e+13 ohm | ASTM D257 |
Supreme Petrochem SP 6411 1924 Light Stabilized Polystyrene Characteristics Prevents dust patterns due to static charges High gloss Good flow Improved light fastness Processing Injection molding Extrusion Applications A/C and cooler grill Material Status.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+13 ohm | 1.00e+12 - 1.00e+13 ohm | ASTM D257 |
Supreme Petrochem SP 6425 9885 Abrasion Resistant Polystyrene Characteristics Low friction, impact polystyrene to provide wear resistance and static charge dissipation Excellent gloss & molded appearance and weld line miscibility Easy flowing grade with good.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+13 ohm | 1.00e+10 - 1.00e+13 ohm | ASTM D257 |
Unitika UNILATE® 1 SC PET Antistatic gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and ot.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+13 ohm | 1.00e+9 - 1.00e+13 ohm | Average value: 1.54e+12 ohm Grade Count:13 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+13 ohm | 1.00e+10 - 1.00e+13 ohm | Average value: 4.31e+12 ohm Grade Count:35 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+13 ohm | 1.00e+10 - 1.00e+13 ohm | Average value: 3.58e+12 ohm Grade Count:14 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+13 ohm @Temperature 90.0 - 90.0 °C |
1.00e+12 - 1.00e+13 ohm @Temperature 194 - 194 °F |
Average value: 5.50e+12 ohm Grade Count:2 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |