| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Rigid Extrusion 87727 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 85 | 85 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 56.9 MPa | 8250 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 2.87 GPa | 416 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 93.5 MPa | 13600 psi | ASTM D790 |
| Flexural Modulus | 2.92 GPa | 424 ksi | ASTM D790 |
| Izod Impact, Notched | 0.450 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.843 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
| Dart Drop Total Energy | 66.3 J/cm @Temperature 23.0 °C |
0.124 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
| 175 J/cm @Temperature 23.0 °C |
0.328 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 61.2 °C @Thickness 3.18 mm |
142 °F @Thickness 0.125 in |
Injection Molded; Annealed; ASTM D648 |
| Flammability, UL94 | V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
TP; UL 94 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 182 - 193 °C | 360 - 379 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Clear/Transparent | |
| Features | General Purpose | |
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Extrusion | |
| PVC Cell Classification | 11553 | ASTM D1784 |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | General Purpose | |
| Profiles |