Covestro Bayblend® FR3012 PC/ABS Blend

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Covestro
Trade Name Bayblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Bayblend® FR3012 PC/ABS Blend.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injection moldingAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 0.20 %
0.20 %
ISO 62, 50% RH
Water Absorption at Saturation 0.50 %
0.50 %
ISO 62
Viscosity 155000 cP

@Shear Rate 1000 1/s,
Temperature 260 °C
155000 cP

@Shear Rate 1000 1/s,
Temperature 500 °F
melt viscosity; b.o. ISO 11443-A
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.00 mm
0.0050 - 0.0070 in/in

@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Thickness 3.00 mm
0.0050 - 0.0070 in/in

@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 60.0 MPa
8700 psi
50 mm/min; ISO 527-1,-2
Elongation at Break >= 40 %
>= 40 %
50 mm/min; b.o. ISO 527-1,-2
Elongation at Yield 3.5 %
3.5 %
50 mm/min; ISO 527-1,-2
Tensile Modulus 2.60 GPa
377 ksi
1 mm/min; ISO 527-1,-2
Izod Impact, Notched (ISO) 10.0 kJ/m²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 180-A
20.0 kJ/m²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 180-A
Izod Impact, Unnotched (ISO) NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 180-U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 76.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
42.2 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ISO 75-1,-2
Vicat Softening Point 100 °C

@Load 5.10 kg
212 °F

@Load 11.2 lb
50°C/h; ISO 306
102 °C

@Load 5.10 kg
216 °F

@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Processing Properties Metric English Comments
Melt Temperature 240 °C
464 °F
Injection molding; ISO 294
Mold Temperature 80.0 °C
176 °F
Injection molding; ISO 294
Injection Velocity 240 mm/sec
9.45 in/sec
ISO 294