| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
| 1.01 g/cc <br>@Temperature 240 °C |
0.0365 lb/in³ <br>@Temperature 464 °F |
Melt | |
| Water Absorption | 0.50 % | 0.50 % | Similar to ISO 62 |
| Moisture Absorption at Equilibrium | 0.20 % | 0.20 % | Similar to ISO 62 |
| Melt Flow | 30 g/10 min <br>@Load 5.00 kg,<br> Temperature 240 °C |
30 g/10 min <br>@Load 11.0 lb,<br> Temperature 464 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 60.0 MPa | 8700 psi | ISO 527-1/-2 |
| Elongation at Yield | 3.5 % | 3.5 % | ISO 527-1/-2 |
| Tensile Modulus | 2.80 GPa | 406 ksi | ISO 527-1/-2 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 76.0 µm/m-°C | 42.2 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
| Specific Heat Capacity | 1.72 J/g-°C | 0.411 BTU/lb-°F | Melt |
| Thermal Conductivity | 0.159 W/m-K | 1.10 BTU-in/hr-ft²-°F | Melt |
| Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ISO 75-1/-2 |
| Vicat Softening Point | 93.0 °C | 199 °F | 50°C/h 50N; ISO 306 |
| Flammability, UL94 | V-0 <br>@Thickness 1.50 mm |
V-0 <br>@Thickness 0.0591 in |
IEC 60695-11-10 |
| 5VB <br>@Thickness 2.00 mm |
5VB <br>@Thickness 0.0787 in |
IEC 60695-11-20 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | IEC 60093 |
| Dielectric Constant | 3.1 <br>@Frequency 1.00e+6 Hz |
3.1 <br>@Frequency 1.00e+6 Hz |
IEC 60250 |
| 3.2 <br>@Frequency 100 Hz |
3.2 <br>@Frequency 100 Hz |
IEC 60250 | |
| Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.0050 <br>@Frequency 100 Hz |
0.0050 <br>@Frequency 100 Hz |
IEC 60250 |
| 0.0065 <br>@Frequency 1.00e+6 Hz |
0.0065 <br>@Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 240 °C | 464 °F | Injection Molding; ISO 294 |
| 240 - 270 °C | 464 - 518 °F | ||
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
| 80.0 °C | 176 °F | Injection Molding; ISO 10724 | |
| Ejection Temperature | 100 °C | 212 °F | |
| Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Availability | Asia Pacific | |
| Europe | ||
| India | ||
| Near East/Africa | ||
| North America | ||
| South and Central America | ||
| Eff. thermal diffusivity (m²/s) | 9.15E-08 | |
| Feature | Release agent | |
| Form | Pellets | |
| Process | Injection Molding |