Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 260 - 288 °C | 500 - 550 °F | |
PolyOne Gravi-Tech™ GRV-NY-030-SS Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
PolyOne Gravi-Tech™ GRV-NY-085-W-NAT Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LGF30 - PA6 Nylon 6, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 30% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LGF40 - PA6 Nylon 6, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Melt Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LGF50 - PA6 Nylon 6, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Melt Temperature | 260 - 288 °C | 500 - 550 °F | |
Polymer Resources PC/TP-GP2-G20 PC/Polyester Alloy, 20% Glass Reinforced Excellent Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Melt Temperature | 260 - 288 °C | 500 - 550 °F | |
Polymer Resources PC/TP-GP3-G10 PC/Polyester Alloy, 10% Glass Reinforced Superior Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Melt Temperature | 260 - 288 °C | 500 - 550 °F | Air purge at equilibrium conditions |
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim |
|||
Melt Temperature | 260 - 288 °C | 500 - 550 °F | |
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Melt Temperature | 260 - 288 °C | 500 - 550 °F | |
PolyOne Gravi-Tech™ GRV-NP-110-W-NAT Polyamide 12 (Nylon 12) Information provided by PolyOne |
|||
Melt Temperature | 249 - 288 °C | 480 - 550 °F | |
Huntsman PE5082 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings (sugar paper and laminations).FDA Notes: Con.. |
|||
Melt Temperature | 260 - 288 °C | 500 - 550 °F | Air purge at equilibrium conditions |
NOVA Chemicals Dylark® 378P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Melt Temperature | 232 - 288 °C | 450 - 550 °F | Average value: 262 °C Grade Count:8 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |
|||
Melt Temperature | 246 - 288 °C | 475 - 550 °F | |
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 246 - 288 °C | 475 - 550 °F | |
Star Plastics PC/ABSFR9002 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 260 - 288 °C | 500 - 550 °F | |
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 260 - 288 °C | 500 - 550 °F | |
Westlake Hifor Xtreme SC74840 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74840 linear low density polyethylene is recommended for the core layer of cast stretch film. It provides excellent clarity and ultimate stretch values higher than the more c.. |
|||
Melt Temperature | 232 - 288 °C | 450 - 550 °F | Extrusion |
Total PPH 3860X Polypropylene, Extrusion Grade High flow reactor grade homopolymer for nonwoven fibersHigh Purity - FINA 3860X features extremely high purity for processing in micro denier fibers.FDA - FINA 3860X complies with all applicable FDA.. |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol 6601FR Nylon 66, Flame Retardant Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol BR2029 Nylon 66, General Purpose, Black Data provided by Clariant Masterbatches |
|||
Melt Temperature | 260 - 288 °C | 500 - 550 °F | |
Clariant Renol PPOSP0001 Polyphenylene Oxide, Mineral Filled Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol 6608 HSL Nylon 66, High Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 271 - 288 °C | 520 - 550 °F | Stock |
PolyOne Edgetek® NI-30GF/000 Nylon 6/10 - 30% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 238 - 288 °C | 460 - 550 °F | |
DuPont Bexloy® AXW604BK 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin
(discontinued **) A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont. |