Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
PolyOne Versaflex™ OM 6258-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6258-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Melt Temperature | 249 - 260 °C | 480 - 500 °F | ASTM D789 |
Niche Polymer PA66MIBK Nylon 66, Medium Impact Information provided by Niche Polymer |
|||
Melt Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Melt Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-G30 Nylon 6, 30% Glass Reinforced Nylon 6, 30% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Melt Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-G43 Nylon 6, 43% Glass Reinforced Nylon 6, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Melt Temperature | 249 - 277 °C | 480 - 530 °F | |
Polymer Resources TP-GFMF1 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame Retardant Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test.. |
|||
Melt Temperature | 249 - 266 °C | 480 - 511 °F | |
LNP VALOX® SMV5845 PBT + PET Alloy, 16% Carbon Fiber Reinforcement
(discontinued **) ESD Applications. Will be VC1600.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.Th.. |
|||
Melt Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-G13-[color]-H Nylon 6, 13% Glass Reinforced, Heat Stabilized Nylon 6, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Melt Temperature | 249 - 271 °C | 480 - 520 °F | Stock |
PolyOne Lubri-Tech™ NL-000/15T Nylon 612 - 15% PTFE Lubricated
(discontinued **) Properties Dry as MoldedData provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. |
|||
Melt Temperature | 249 - 260 °C | 480 - 500 °F | |
Firestone CL200-001 Nylon 6 Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Melt Temperature | 249 - 260 °C | 480 - 500 °F | |
Firestone CLM200-001 Nylon 6 Used for monofiliament extrusion. Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
Eastman Drystar 0325 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
Eastman Eastar DN011 Copolyester Eastar Copolyester DN011 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN011 contains a mold release.Applications/.. |
|||
Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
Eastman Eastar MN210 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates.Applications/UsesMedical |
|||
Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
Eastman Eastar MN211 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. MN211 contains a mold release.Application.. |
|||
Melt Temperature | 249 - 282 °C | 480 - 540 °F | |
Clariant PA213N40 Nylon 6, Mineral/Glass Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 249 - 277 °C | 480 - 530 °F | |
Clariant Renol 60G13HSP Black Nylon 6, 13% Glass Fiber Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 249 - 277 °C | 480 - 530 °F | |
Clariant Renol PA233HT Nylon 6, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Melt Temperature | 249 °C | 480 °F | |
Chem Polymer Chemlon 223 Nylon 6, Nucleated A highly nucleated, lubricated nylon 6 intended for applications requiring a faster cycle time. It has increased tensile strength, rigidity, creep resistance and hardness over general purpose nylon.. |
|||
Melt Temperature | 249 - 316 °C | 480 - 600 °F | Average value: 287 °C Grade Count:11 |