| Category | Polymer , Thermoplastic , Nylon , Nylon 610 , Nylon 610, Glass Reinforced |
| Manufacturer | |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Edgetek® NI-30GF/000 Nylon 6/10 - 30% Glass Fiber Reinforced
(discontinued **).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.31 g/cc | 0.0473 lb/in³ | ASTM D792 |
| Water Absorption | 0.20 % | 0.20 % | 24 hrs. ASTM D570 |
| Linear Mold Shrinkage | 0.0030 cm/cm <br>@Thickness 3.17 mm |
0.0030 in/in <br>@Thickness 0.125 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 119 | 119 | ASTM D785 |
| Tensile Strength, Ultimate | 145 MPa | 21000 psi | ASTM D638 |
| Elongation at Break | 3.0 - 4.0 % | 3.0 - 4.0 % | ASTM D638 |
| Flexural Yield Strength | 221 MPa | 32100 psi | ASTM D790 |
| Flexural Modulus | 7.60 GPa | 1100 ksi | ASTM D790 |
| Compressive Yield Strength | 123 MPa | 17800 psi | ASTM D695 |
| Shear Strength | 72.0 MPa | 10400 psi | ASTM D732 |
| Izod Impact, Notched | 1.71 J/cm <br>@Thickness 6.35 mm |
3.20 ft-lb/in <br>@Thickness 0.250 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 28.8 µm/m-°C <br>@Temperature 20.0 °C |
16.0 µin/in-°F <br>@Temperature 68.0 °F |
ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 421 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 271 - 288 °C | 520 - 550 °F | Stock |
| Mold Temperature | 93.0 - 107 °C | 199 - 225 °F | |
| Drying Temperature | 82.0 °C | 180 °F |