| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 2.99 g/cc | 2.99 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 68.3 MPa | 9910 psi | Type I, 5.1 mm/min; ASTM D638 |
| Elongation at Break | 1.7 % | 1.7 % | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 7.24 GPa | 1050 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Modulus | 5.72 GPa | 830 ksi | ASTM D790 |
| Izod Impact, Notched | 0.530 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 149 °C @Thickness 6.35 mm |
300 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 260 - 288 °C | 500 - 550 °F | |
| Mold Temperature | 82.2 - 149 °C | 180 - 300 °F | |
| Drying Temperature | 79.4 °C | 175 °F | |
| Dry Time | 4.00 hour | 4.00 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Non-Toxic | |
| Forms | Pellets | |
| Generic Material | Nylon 6 | |
| Generic Name | Polyamide 6 (Nylon 6) | |
| Processing Method | Injection Molding | |
| Regional Availability | Asia Pacific | |
| Uses | Industrial Applications | |
| Medical/Healthcare Applications | ||
| Projectiles | ||
| Sporting Goods | ||
| Weighting & Balancing |