| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
|
Polymer Resources PC-FD4-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
|
|||
| Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
|
Polymer Resources PC-GP4-[color]-3 Polycarbonate, UV-stabilized, Easy Flow
Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P..
|
|||
| Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
|
Polymer Resources PC-GP4-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Easy Flow
Polycarbonate, FDA-compliant Feedstocks, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
|
Polymer Resources PC-UV4 Polycarbonate, UV-stabilized, Easy Flow
Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P..
|
|||
| Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
|
Polymer Resources PC-UV4-[color]-1 Polycarbonate, UV-stabilized, Easy Flow with Mold Release
Polycarbonate, UV-stabilized, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
|
|||
| Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
|
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6
(discontinued **)
Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B..
|
|||
| Melt Temperature | 266 - 282 °C | 510 - 540 °F | |
|
MRC Polymers NAXALOYâ„¢ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled
Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc.
|
|||
| Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
|
MTI ThermoStran® PA66-40C Long Carbon Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
|
|||
| Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
|
MTI ThermoStran® PA66-40G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
|
|||
| Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
|
MTI ThermoStran® PA66-50G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
|
|||
| Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
|
MTI ThermoStran® PA66-60G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
|
|||
| Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
|
Clariant 6602-L BK-02 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
|
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
|
Clariant PA131G2GN-91 Green Nylon 66, Highly Toughened
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
|
Clariant Renol BR2029 Nylon 66, General Purpose, Black
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
|
Clariant Renol BRU0000BN-182 Nylon 66, Lubricated, Nucleated, Weather Resistant
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
|
Clariant Renol PA101F/ST801 Nylon 66, Impact Modified, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
|
Clariant Renol PA101LRD-190 Nylon 66, General Purpose, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
|
Clariant Renol PA112 Nylon 66, Nucleated
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
|
Clariant Renol PA113 Nylon 66, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
|
Clariant Renol PA113C Nylon 66, Molybdenum Disulfide Lubricated
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
|
Clariant Renol PA123 Nylon 66, Impact Modified, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
|
Clariant Renol PA133 Nylon 66, Highly Impact Modified, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
|
Clariant Renol PA133GN-109 Nylon 66, High Impact, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
|
Clariant Renol PA611D40 Nylon 612, Glass Fiber Reinforced, Molybdenum Disulfide Lubricated
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
|
Clariant Renol 6608 HSL Nylon 66, High Impact Modified, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
|
Clariant Renol 6608-L Nylon 66, High Impact Modified, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
|
Clariant Renol PA113G33 Nylon 66, 33% Glass Fiber, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||