Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
PolyOne Versaflex™ OM 6258-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6258-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Melt Temperature | 243 - 271 °C | 470 - 520 °F | |
Ravago Manufacturing Americas Hylon® N2000STL Nylon 6 (DAM) Information provided by Ravago. |
|||
Melt Temperature | 249 - 271 °C | 480 - 520 °F | Molding |
PolyOne Lubri-Tech™ PS-15GB/10T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated
(discont Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 238 - 271 °C | 460 - 520 °F | Molding |
PolyOne Lubri-Tech™ PS-30GF/02S Polybutylene Terephthalate (PBT), Glass Filled, PTFE/Silicone Lubricated
(dis Description/Features:Glass Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 243 - 271 °C | 470 - 520 °F | Molding |
PolyOne Lubri-Tech™ PS-30GF/10T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated
(discontinued Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 232 - 271 °C | 450 - 520 °F | Molding |
PolyOne Edgetek® BB-25GF/000 PC/ABS Blend, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 232 - 271 °C | 450 - 520 °F | Air purge at equilibrium conditions |
NOVA Chemicals Dylark® 510XT Glass Reinforced Engineering Resin Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri.. |
|||
Melt Temperature | 238 - 271 °C | 460 - 520 °F | Stock |
PolyOne Edgetek® NJ-10GF/000 Nylon 12 - 10% Glass Fiber
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 249 - 271 °C | 480 - 520 °F | Stock |
PolyOne Lubri-Tech™ NL-000/15T Nylon 612 - 15% PTFE Lubricated
(discontinued **) Properties Dry as MoldedData provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. |
|||
Melt Temperature | 238 - 271 °C | 460 - 520 °F | Stock |
PolyOne Lubri-Tech™ NL-10GF/15TF Nylon 6/12 - 10% Glass Fiber - 15% PTFE Flock
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 238 - 271 °C | 460 - 520 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
MRC Polymers NAXALOYâ„¢ 780 PC+PBT Polyester Blend Good chemical resistance, impact and heat resistance.Information provided by MRC Polymers Inc. |
|||
Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
Eastman Eastar MN210 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates.Applications/UsesMedical |
|||
Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
Clariant 6004G13-HSL BK UV Black Nylon 6, 13% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
Clariant 6008 L Nylon 6, High Impact, Injection Molding Data provided by Clariant Masterbatches |
|||
Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
Clariant Renol 6253 Nylon 6, High Impact Data provided by Clariant Masterbatches |