Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 200 - 230 °C | 392 - 446 °F | |
PolyOne OnFlex™ S KE 60A-3S1725 Thermoplastic Elastomer (TPE) OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | |
Polykemi AB POLYabs S00 ABS, High Flow Information provided by Polykemi AB |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | |
Polykemi AB POLYelast TPE EC88R Thermoplastic Elastomer, PP/EPDM Information provided by Polykemi AB |
|||
Melt Temperature | 160 - 230 °C | 320 - 446 °F | |
NOVA Chemicals Novapol® GI-3526-A LLDPE Masterbatch Resin Molded Plaque Properties. Features: High flow, Granular, Improved dispersion concentrates.Applications: housewares, additive and color, masterbatches/compounding.Data provided by the manufacturer. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | |
NOVA Chemicals Sclair® 19G Homopolymer HDPE Film Resin Features: Excellent barrier propertiesHigh stiffnessGood processability Low gel Applications: Barrier filmsCo-extrusionDry food packagingInformation provided by Nova Chemicals |
|||
Melt Temperature | 180 - 230 °C | 356 - 446 °F | |
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **) PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Melt Temperature | 170 - 230 °C | 338 - 446 °F | |
NOVA Chemicals Sclair® 2710 HDPE Injection Molding Resin Features: Good ESCR, good processability.Applications: Housewares, containers, toys.Data provided by the manufacturer. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL HI5302RB PP+MF25%, High Impact Description: Injection Molding, PP+MF25%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL TE5107 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Melt Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical MP211 ABS, Low Gloss, Metal Plating Feature: Injection Molding, High Flow, Metal PlatingApplication: Decorative Parts (Home Appliance Door Handle Etc)CAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion |
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA) High-impact grade of polystyrene with improved impact strength and heat resistance, developed for injection molding and extrusion/thermoforming applications.Information provided by BASF.Ineos Styren.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion |
Ineos Styrenics Polystyrene 476M (NAFTA) High-impact grade of polystyrene with good ESCR designed to provide uniform melt flow for excellent processability.Information provided by BASF.Ineos Styrenics purchased this product line from BASF .. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | |
Lavergne VYSTYRENE PS 3904 High Impact Polystyrene Vystyrene PS 3904 is a black impact modified polystyrene compound with balanced impact/stiffness properties designed for injection molding applicationsFeatures: -High resilience -Excellent process.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL HF3308C PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Che.. |
|||
Melt Temperature | 150 - 230 °C | 302 - 446 °F | Injection Molding |
Stellarchem GP-860HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Melt Temperature | 150 - 230 °C | 302 - 446 °F | Extrusion |
Stellarchem GP-965B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Melt Temperature | 210 - 230 °C | 410 - 446 °F | |
Borealis Beta-PPR™ RA7050 Polypropylene-Random-Copolymer for Pressure Pipe Systems Beta-PPR RA7050 is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof of t.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Processing Temperature |
Teknor Apex Uniprene® UN-1373G Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Processing Temperature |
Teknor Apex Uniprene® UN-1674C Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Processing Temperature |
Teknor Apex Uniprene® UN-2598E Thermoplastic Vulcanizate Alloy Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Processing Temperature |
Teknor Apex Uniprene® UN-7200-73 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Automotive Specifications: Chrysler MS-AK91; FORD WSS-M2D510-A7; .. |
|||
Melt Temperature | 220 - 230 °C | 428 - 446 °F | |
Tisan TISESTER® 30% Glass Fiber Reinforced Heat Stabilized Copolymer Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Melt Temperature | 180 - 230 °C | 356 - 446 °F | |
Advanced Polymer Alloys DuraGrip™ 6165 TR Thermoplastic Elastomer DuraGrip® DGR6165TR is a translucent thermoplastic elastomer (TPE) formulated for excellent elastic properties and enhanced adhesion to engineered thermoplastics using insert molding, co-injection .. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LI912 ASA Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical |
|||
Melt Temperature | 220 - 230 °C | 428 - 446 °F | |
NOVA Chemicals Sclair® 11H1 LLDPE Film Resin
(discontinued **) Low gel, Excellent heat sealability, Easy processability, High toughness and strengthApplications: Heavy duty sack, High strength packagingAdditives: Process stabilizer, Polymer process aid, Antiblo.. |