| Category | Polymer , Thermoplastic , Elastomer, TPE , Polypropylene (PP) |
| Manufacturer | Polykemi AB |
| Trade Name | POLYelast |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Polykemi AB POLYelast TPE EC88R Thermoplastic Elastomer, PP/EPDM.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | With Flow; ISO 2577 |
| 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | Across Flow; ISO 2577 | |
| Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 88 @Time 15.0 sec |
88 @Time 0.00417 hour |
Polykemi |
| Hardness, Shore D | 30 @Time 15.0 sec |
30 @Time 0.00417 hour |
Polykemi |
| Tensile Strength at Break | <= 15.0 MPa | <= 2180 psi | ISO/R527 |
| Elongation at Break | >= 55 % | >= 55 % | ISO/R527 |
| Flexural Modulus | 0.450 GPa @Temperature 23.0 °C |
65.3 ksi @Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179 |
| NB @Temperature -20.0 °C |
NB @Temperature -4.00 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 56.0 °C | 133 °F | 120°C/h; ISO 75/1 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 200 - 230 °C | 392 - 446 °F | |
| Mold Temperature | 20.0 - 60.0 °C | 68.0 - 140 °F | |
| Injection Pressure | 90.0 - 110 MPa | 13100 - 16000 psi | |
| Back Pressure | 0.200 - 0.500 MPa | 29.0 - 72.5 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Holding Pressure () | 20-40 | % of injection pressure |
| Injection Speed () | High |