Polymer Property : Melt Temperature = 170 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 170 - 190 °C
338 - 374 °F
Plastcom SLOVALEN EH 96 FRD 2 PP, flame retardant
FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin..
Melt Temperature 170 - 210 °C
338 - 410 °F
PolyOne OnFlex™ U 5365A-E0134 FG Thermoplastic Elastomer (TPE)
OnFlex™ U 5365A-E0134 FG is a performance TPU alloy designed for use in injection molding application where FDA compliance and Overmolding onto PC, ABS and PC/ABS substrates are required.Properties..
Melt Temperature 170 - 210 °C
338 - 410 °F
PolyOne OnFlex™ U 5380A-S0013 Thermoplastic Elastomer (TPE)
OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of..
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 59A HDPE Injection Molding Resin
Features: Homopolymer, high drop impact resistance and high stiffness.Applications: Juice, water containers, personal protective equipment, grain elevator buckets, designed for accumulator and recip..
Melt Temperature 170 - 282 °C
338 - 540 °F
Average value: 219 °C Grade Count:44
Overview of materials for Polystyrene, Transparent Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of..
Melt Temperature 170 - 220 °C
338 - 428 °F
Lotte Chemical Titan TITANEX® LI2516 Linear low density polyethylene resin  (discontinued **)
LI2516 is a pelleted linear low density polyethylene with very narrow molecular weight distribution.Applications: House-wares, lids, closures and toys.Advantages: Excellent stress crack resistance,..
Melt Temperature 170 - 190 °C
338 - 374 °F
NOVA Chemicals Novapol® LF-0218-AB LDPE Film Resin  (discontinued **)
Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu..
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 58G (High Gloss) HDPE Blow Molding Resin  (discontinued **)
Features: Outstanding gloss, pearlescent finish when colored, good processability.Applications: Small part blow molding, injection blow molding, low-moderate ESCR uses.Data provided by the manufactu..
Melt Temperature 170 - 260 °C
338 - 500 °F
NOVA Chemicals Sclair® 2717 HDPE Injection Molding Resin  (discontinued **)
Features: Super high flow, good balance of toughness and stiffness, low odor, permits container weight reduction.Applications: Thin walled food containers.Data provided by the manufacturer.
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 2607 HDPE Injection Molding Resin
Features: Excellent stiffness, good impact resistance, low warpage.Applications: Roll-out carts.Data provided by the manufacturer.
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 2709 HDPE Injection Molding Resin
Features: Excellent cold temperature toughness, high stiffness.Applications: Housewares, containers, pails, closures.Data provided by the manufacturer.
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 8107G UV8D Butene LLDPE Rotational Molding Resin
Excellent ESCR, Excellent low temperature impact properties, Excellent low shrinkage and warpage properties, Very good processability, UL 94-HB listedApplications: Food and laundry materials handlin..
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 2508-UV9 MDPE Injection Molding Resin  (discontinued **)
Features: Excellent processability for applications requiring stiffness and toughness, good cold temperature impact properties.Applications: Roll-out cart lids.Data provided by the manufacturer.
Melt Temperature 170 - 302 °C
338 - 576 °F
Average value: 215 °C Grade Count:17
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
Melt Temperature 170 - 195 °C
338 - 383 °F
Injection
Huntsman IROGRAN® A 87 H 4615 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 87 H 4615 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi..
Melt Temperature 170 - 195 °C
338 - 383 °F
Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry
Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and lo..
Melt Temperature 170 - 210 °C
338 - 410 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1030D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Melt Temperature 170 - 210 °C
338 - 410 °F
Injection Molding
Stellarchem LP-830 TPE Compound
This grade of Stellarchem LP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, ..
Melt Temperature 170 - 200 °C
338 - 392 °F
Borealis BS2581 High Density Polyethylene for Blow Molding
BS2581 is a high density polyethylene intended for blow molding products with high stiffness and very good environmental stress crack resistance (ESCR). Applications: industrial chemicals, househol..
Melt Temperature 170 - 180 °C
338 - 356 °F
DuPont Elvaloy® 3217 AC Ethylene and 17% Butyl Acrylate Copolymer
Elvaloy® 3217 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3217 AC has been developed for film applications requiring a combination of softness, toughness and low friction. Typi..
Melt Temperature 170 - 190 °C
338 - 374 °F
Tisan TISOPLEN® 10% Calcite Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Melt Temperature 170 - 190 °C
338 - 374 °F
Tisan TISOPLEN® 30% Glass Fiber Reinforced Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Melt Temperature 170 °C
338 °F
Lubrizol Estane® ALR G500 Water Absorbent Thermoplastic Polyurethane
Type: Estane® ALR G500 is an aliphatic thermoplastic polyurethane (TPU) resin designed to absorb water and transport moisture.Features: Contains UV additivesAvailable in AmericasInformation Provide..
Melt Temperature 170 °C
338 °F
Carmel Olefins IPETHENE® 210 Low Density Polyethylene
IPETHENE® 210 is a low density polyethylene extrusion grade, containing no additives. It exhibits a good balance between mechanical and optical properties. APPLICATIONS IPETHENE® 210 is mainly u..
Melt Temperature 170 °C
338 °F
Carmel Olefins IPETHENE® 213 Low Density Polyethylene
IPETHENE® 213 is a general purpose low density polyethylene film extrusion grade. It contains a medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between ..
Melt Temperature 170 - 220 °C
338 - 428 °F
Average value: 200 °C Grade Count:14
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Melt Temperature 170 - 250 °C
338 - 482 °F
Average value: 225 °C Grade Count:8
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
Melt Temperature 170 - 279 °C
338 - 534 °F
Average value: 224 °C Grade Count:92
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
Melt Temperature 170 - 260 °C
338 - 500 °F
NOVA Chemicals Sclair® 2715 HDPE Injection Molding Resin  (discontinued **)
Features: Excellent low temperature impact strength, good balance of toughness and stiffness, low odor.Applications: Thin walled food containers and lids, frozen and refrigerated containers.Data pro..
Melt Temperature 170 - 260 °C
338 - 500 °F
NOVA Chemicals Sclair® 2915 HDPE Injection Molding Resin  (discontinued **)
Features: Excellent balance of stiffness and toughness, low odor, permits light weight container design.Applications: Thin walled food containers, frozen food containers.Data provided by the manufac..