Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 204 - 227 °C | 399 - 441 °F | |
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene.. |
|||
Melt Temperature | 204 - 227 °C | 399 - 441 °F | |
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene.. |
|||
Melt Temperature | 204 - 227 °C | 399 - 441 °F | |
PolyOne Versaflex™ FFC 2882-87 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-87 is designed to pass several fatty food extraction conditions identified in EU Directive 2002/72/EC, FDA 21 CFR 177.2600, and GB 4806.1-94. Versaflex™ FFC 2882-87 will also o.. |
|||
Melt Temperature | 204 - 227 °C | 399 - 441 °F | |
PolyOne Versaflex™ FFC 2882-87 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-87 is designed to pass several fatty food extraction conditions identified in EU Directive 2002/72/EC, FDA 21 CFR 177.2600, and GB 4806.1-94. Versaflex™ FFC 2882-87 will also o.. |
|||
Melt Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Versaflex™ OM 1060X-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 1060X-9 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Excellent Bond to PC, ABS, PC/ABS - Good Surface Aesthetics - Rubbery Feel - Soft TouchPurge thoro.. |
|||
Melt Temperature | 216 - 227 °C | 420 - 441 °F | ASTM D789 |
Niche Polymer PA6BK Nylon 6 Information provided by Niche Polymer |
|||
Melt Temperature | 216 - 227 °C | 420 - 441 °F | ASTM D789 |
Niche Polymer PA6GF13BK Nylon 6, 13% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 216 - 227 °C | 420 - 441 °F | ASTM D789 |
Niche Polymer PA6GF13N Nylon 6, 13% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 216 - 227 °C | 420 - 441 °F | ASTM D789 |
Niche Polymer PA6GF43BK Nylon 6, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 216 - 227 °C | 420 - 441 °F | ASTM D789 |
Niche Polymer PA6GF43N Nylon 6, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 216 - 227 °C | 420 - 441 °F | ASTM D789 |
Niche Polymer PA6GF50BK Nylon 6, 50% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 216 - 227 °C | 420 - 441 °F | ASTM D789 |
Niche Polymer PA6GM40BK Nylon 6, 40% Mineral Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynalloy™ OBC8000-T40 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T40 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl.. |
|||
Melt Temperature | 204 - 227 °C | 399 - 441 °F | |
PolyOne Edgetek® AT-1000 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Temperature | 150 - 227 °C | 302 - 441 °F | Average value: 191 °C Grade Count:79 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Melt Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynalloy™ OBC8000-T60 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T60 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl.. |
|||
Melt Temperature | 210 - 227 °C | 410 - 441 °F | Molding |
Lubrizol Pellethane® 2363-65D Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Melt Temperature | 210 - 227 °C | 410 - 441 °F | Molding |
Lubrizol Pellethane® 2363-75D Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Melt Temperature | 193 - 227 °C | 379 - 441 °F | |
Total PPR Z9421 Polypropylene, Random Copolymer, Heat Sealable Film Grade Color/Clarity/Impact. TOTAL Petrochemicals Polypropylene Z9421 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable. The very low melting.. |
|||
Melt Temperature | 210 - 227 °C | 410 - 441 °F | Molding |
Lubrizol Estane® 2103-55D Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Load bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in .. |
|||
Melt Temperature | 199 - 227 °C | 390 - 441 °F | |
Bapolene® 222F Polyethylene, Film Grade Bapolene LL222F is a general purpose LLDPE for blown film extrusion or cast film applications. This resin offers excellent tensile and toughness properties. It is available with and without slip/a.. |
|||
Melt Temperature | 204 - 227 °C | 399 - 441 °F | |
Ineos Nova 8048 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Improved toughness, Custom colorsApplications: Designed for injection molding applications requiring clarity and toughnessPerformance grades of polystyrene are engineered to have specific properties.. |
|||
Melt Temperature | 204 - 227 °C | 399 - 441 °F | |
Ineos Nova 817 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow crystal polystyrene, Custom colorsApplications: Injection molding, Designed for use in high speed, Thin section applications and complex parts designs where custom coloring is a requiremen.. |
|||
Melt Temperature | 188 - 227 °C | 370 - 441 °F | Stock |
PolyOne Edgetek® AT-000/07SS Copolymer Acetal - 7% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 210 - 227 °C | 410 - 441 °F | |
Dow PELLETHANE® 2103-75D Film Grade Thermoplastic Polyurethane Elastomer
(discontinued **) Description: PELLETHANE® 2103-75D UV stabilized, polyether based thermoplastic polyurethane elastomer has excellent hydrolytic stability and excellent resistance to micro-organisms. Applications in.. |
|||
Melt Temperature | 210 - 227 °C | 410 - 441 °F | |
Dow PELLETHANE® 2104-65D Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2104-65D Polyester based. Excellent oil and chemical resistance. Applications include: Caster wheels, Seals, Gaskets, Animal tags, Hose jacketing, Ski boots, AutomotiveDat.. |
|||
Melt Temperature | 210 - 227 °C | 410 - 441 °F | |
Dow PELLETHANE® 2104-45D Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2104-45D ether-ether hybrid polyurethane elastomer has excellent low temperature properties, fast cycle time, and good resistance to fuel and oils. Applications include: C.. |