| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 10% Glass Fiber Filled |
| Manufacturer | Niche Polymer |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Niche Polymer PA6GF13N Nylon 6, 13% Glass Fiber Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.00550 cm/cm | 0.00550 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D638 |
| Elongation at Break | 5.00 % | 5.00 % | ASTM D638 |
| Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
| Flexural Modulus | 4.83 GPa | 700 ksi | ASTM D790 |
| Izod Impact, Unnotched | 0.481 J/cm <br>@Thickness 3.17 mm |
0.900 ft-lb/in <br>@Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 193 °C | 380 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 216 - 227 °C | 420 - 441 °F | ASTM D789 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Natural |