| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced |
| Manufacturer | Niche Polymer |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Niche Polymer PA6BK Nylon 6.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.0130 cm/cm | 0.0130 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 75.8 MPa | 11000 psi | ASTM D638 |
| Elongation at Break | 60.0 % | 60.0 % | ASTM D638 |
| Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
| Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
| Izod Impact, Unnotched | 0.587 J/cm @Thickness 3.17 mm |
1.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 64.00 °C | 147.2 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 216 - 227 °C | 420 - 441 °F | ASTM D789 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Black |