Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
Polymer Resources PC/ASA-GP2 Polycarbonate/ASA Alloy Acrylonitrile Styrene Acrylate + PolycarbonatePreliminary DataProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
Melt Temperature | 254 - 277 °C | 490 - 530 °F | |
Ravago Manufacturing Americas Hylon® N2015L Nylon 6 (Cond) Information provided by Ravago. |
|||
Melt Temperature | 254 - 277 °C | 490 - 530 °F | |
Ravago Manufacturing Americas Hylon® N2017THL Nylon 6 (DAM) Information provided by Ravago. |
|||
Melt Temperature | 254 - 277 °C | 490 - 530 °F | |
Ravago Manufacturing Americas Hylon® N2033HL Nylon 6 (DAM) Information provided by Ravago. |
|||
Melt Temperature | 254 - 277 °C | 490 - 530 °F | |
Ravago Manufacturing Americas Hylon® N2033THL Nylon 6 (DAM) Information provided by Ravago. |
|||
Melt Temperature | 254 - 277 °C | 490 - 530 °F | |
Ravago Manufacturing Americas Hylon® N2017STHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Melt Temperature | 254 - 338 °C | 490 - 640 °F | Average value: 296 °C Grade Count:7 |
Overview of materials for Polycarbonate, Foam Grade, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Melt Temperature | 254 - 282 °C | 490 - 540 °F | Molding |
PolyOne Lubri-Tech™ NL-30GF/15T Nylon 6/12, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)Information provided by PolyOne Corporation. |
|||
Melt Temperature | 254 - 277 °C | 490 - 530 °F | |
LTL Color Compounds ColorFast® FRPBT130 PBT, 30% Glass-Filled 30% glass-filled V-0 rated PBT - UL listedAll information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 254 - 277 °C | 490 - 530 °F | |
LTL Color Compounds ColorFast® FRPBT150 PBT, 13% Glass-Filled, Flame Retarded 13% glass-filled V-0 rated PBTAll information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
MRC Polymers NAXELLâ„¢ PC23MS Polycarbonate, Impact Modified, High MFR, EZ Flow Economy GradeImpact modifiedCan be UV stabilizedGenerally for black onlyInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Melt Temperature | 254 - 282 °C | 490 - 540 °F | |
Wellman Wellamid® GF14-60 XE-N 14% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Melt Temperature | 254 - 282 °C | 490 - 540 °F | |
Wellman Wellamid® GF20-60 XE-N 20% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Melt Temperature | 254 - 282 °C | 490 - 540 °F | |
Wellman Wellamid® GF30-60 XE-N 30% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
Clariant 6004G13-HSL BK UV Black Nylon 6, 13% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
Clariant 6004G8-HSL BK UV Black Nylon 6, 8% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
Clariant 6008 L Nylon 6, High Impact, Injection Molding Data provided by Clariant Masterbatches |
|||
Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
Clariant PA213M40 Nylon 6, 40% Mineral Reinforced, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black Data provided by Clariant Masterbatches |
|||
Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
Clariant Renol 6001 HV HSL Nylon 6, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
Clariant Renol 6253-L UV Nylon 6, High Impact, Lubricated, UV Stabilized Data provided by Clariant Masterbatches |
|||
Melt Temperature | 254 - 282 °C | 490 - 540 °F | |
Clariant Renol BR7140 Polycarbonate/ABS Alloy Data provided by Clariant Masterbatches |
|||
Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
Clariant Renol PA2SP0017 Nylon 6, Impact Modified Data provided by Clariant Masterbatches |
|||
Melt Temperature | 254 - 282 °C | 490 - 540 °F | |
Clariant Renol PCSP0007 Polycarbonate/Polyester Alloy Data provided by Clariant Masterbatches |
|||
Melt Temperature | 254 - 282 °C | 490 - 540 °F | |
Clariant Renol PCSP0016BL-201 Polycarbonate/Polyester Alloy Data provided by Clariant Masterbatches |
|||
Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
Clariant PA223 Nylon 6, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 254 °C | 490 °F | |
Teknor Apex Chemlon® 109-18 GH Nylon 66, 18% Glass Fiber Reinforced Notes: High-impact; Reinforced with 18% glass fibers; Highly toughened compound designed to improve practical toughness and ductility Features: Ductile; Good Impact Resistance; Good Toughness; Good .. |