Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 254 - 266 °C | 489 - 511 °F | ASTM D789 |
Niche Polymer PA66BK Nylon 66 Information provided by Niche Polymer |
|||
Melt Temperature | 254 - 266 °C | 489 - 511 °F | ASTM D789 |
Niche Polymer PA66GF33BK Nylon 66, 33% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 254 - 266 °C | 489 - 511 °F | ASTM D789 |
Niche Polymer PA66GF43N Nylon 66, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 254 - 266 °C | 489 - 511 °F | ASTM D789 |
Niche Polymer PA66GF50BK Nylon 66, 50% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 254 - 271 °C | 489 - 520 °F | ASTM D789 |
Niche Polymer PA66GM38BK Nylon 66, 38% Glass/Mineral Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 254 - 266 °C | 489 - 511 °F | ASTM D789 |
Niche Polymer PA66GM40N Nylon 66, 40% Mineral Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 254 - 327 °C | 489 - 621 °F | Average value: 296 °C Grade Count:36 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Melt Temperature | 254 - 260 °C | 489 - 500 °F | Tubular (Blown) Film |
Honeywell Aegis™ H73MP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H73MP is a lubricated nucleated low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR .. |
|||
Melt Temperature | 254 - 260 °C | 489 - 500 °F | Tubular (Blown) Film |
Honeywell Aegis™ H85ZP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H85ZP is a medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well as EU.. |
|||
Melt Temperature | 254 - 260 °C | 489 - 500 °F | Tubular (Blown) Film |
Honeywell Aegis™ H135KQP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H135KQP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to applicable FDA requirements, including 21 CFR 177.1500 for N6 an.. |
|||
Melt Temperature | 254 - 260 °C | 489 - 500 °F | Tubular (Blown) Film |
Honeywell Aegis™ H135XP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H135XP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Melt Temperature | 254 - 260 °C | 489 - 500 °F | Tubular (Blown) Film |
Honeywell Aegis™ H205QP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H205QP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500. It possesses the combination.. |
|||
Melt Temperature | 254 - 260 °C | 489 - 500 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 .. |
|||
Melt Temperature | 254 - 260 °C | 489 - 500 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H100QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100QP is a lubricated medium viscosity, Nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500 as well as EU Directiv.. |
|||
Melt Temperature | 254 - 260 °C | 489 - 500 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H100ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100ZP is a medium viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well .. |
|||
Melt Temperature | 254 - 260 °C | 489 - 500 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Melt Temperature | 254 - 260 °C | 489 - 500 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H135QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135QP is a lubricated high viscosity, N6, film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements including, 21 CFR 177.1500 as well as EU Direct.. |
|||
Melt Temperature | 254 - 260 °C | 489 - 500 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Melt Temperature | 254 - 260 °C | 489 - 500 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H155MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H155MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Melt Temperature | 254 - 260 °C | 489 - 500 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E.. |
|||
Melt Temperature | 254 - 260 °C | 489 - 500 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H85QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H85QP is a lubricated, medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 a.. |
|||
Melt Temperature | 254 °C | 489 °F | |
Chem Polymer Chemlon 217 GI Nylon 6, 17% Glass Fiber Reinforced A 17% glass fiber reinforced, impact modified nylon 6 offering a combination of creep resistance, stiffness and toughness over unmodified nylon 6 materials.Data provided by the manufacturer, Chem Po.. |
|||
Melt Temperature | 254 °C | 489 °F | |
Chem Polymer Chemlon 225 G Nylon 6, 25% Glass Fiber Reinforced A 25% glass fiber reinforced nylon 6 offering a balance of properties between the 20% (Chemlon 220 G) and 30% (Chemlon 233 G) product offerings. This product offers further improvements in tensile .. |
|||
Melt Temperature | 254 °C | 489 °F | |
Chem Polymer Chemlon 225-15 MG Nylon 6, 25% Mineral/15% Glass Fiber Reinforced A 25% mineral reinforced, 15% glass fiber reinforced nylon 6 offering excellent rigidity, dimensional stability and warpage control in large area parts.Data provided by the manufacturer, Chem Polyme.. |
|||
Melt Temperature | 254 °C | 489 °F | |
Chem Polymer Chemlon 233 G Nylon 6, 33% Glass Fiber Reinforced A 33% glass fiber reinforced nylon 6 offering excellent high temperature performance, dimensional stability, tensile strength and impact resistance.Data provided by the manufacturer, Chem Polymer. |
|||
Melt Temperature | 254 °C | 489 °F | |
Chem Polymer Chemlon 240 G Nylon 6, 43% Glass Fiber Reinforced A 43% glass fiber reinforced nylon 6, offering high rigidity and tensile strength, especially at high service temperatures.Data provided by the manufacturer, Chem Polymer. |
|||
Melt Temperature | 254 °C | 489 °F | |
Chem Polymer Durlex 715 G PBT, 15% Glass Reinforced A lubricated, 15% glass reinforced PBT offering a balance of rigidity, dimensional stability and toughness.Data provided by the manufacturer, Chem Polymer. |
|||
Melt Temperature | 254 °C | 489 °F | |
Chem Polymer Durlex 730 G PBT, 30% Glass Fiber Reinforced A lubricated 30% glass reinforced PBT offering a balance of dimensional stability, tensile strength and high temperature performance.Data provided by the manufacturer, Chem Polymer. |
|||
Melt Temperature | 254 °C | 489 °F | |
Chem Polymer Durlex 730 GVH PBT, 30% Glass Fiber Reinforced A glass fiber reinforced, flame retardant PBT exhibiting excellent strength, dimensional stability and elevated temperature performance. The material has a V0 flammability rating according to UL94 .. |
|||
Melt Temperature | 254 - 277 °C | 489 - 531 °F | |
PolyOne Stat-Tech™ NJ-20CF/000 Black Polyamide 12 (Nylon 12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |