Material Notes:
A 25% mineral reinforced, 15% glass fiber reinforced nylon 6 offering excellent rigidity, dimensional stability and warpage control in large area parts.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 128 MPa
18600 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 193 MPa
28000 psi
ASTM D790
Flexural Modulus 7.60 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
405 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 254 °C
489 °F