Polymer Property : Melt Temperature = 305 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 285 - 305 °C
545 - 581 °F
DAM
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66  (Unverified Data**)
Zytel® 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Melt Temperature 285 - 305 °C
545 - 581 °F
DAM
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66  (Unverified Data**)
Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers
Melt Temperature 285 - 305 °C
545 - 581 °F
DAM
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66  (Unverified Data**)
Zytel® 80G14AHS BK099 is a 14% glass fiber reinforced, toughened, high flow, heat stabilized, black polyamide 66 resin. It offers outstanding performance in injection molding applications.Informati..
Melt Temperature 285 - 305 °C
545 - 581 °F
Solvay Specialty Polymers Kalix® 9950 Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 9950 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties and excellent surface ..
Melt Temperature 295 - 305 °C
563 - 581 °F
A. Schulman SCHULAMID® 66 MK30HI 30% Mineral Reinforced, Impact Modified Nylon 66
Information provided by A. Schulman.
Melt Temperature 280 - 305 °C
536 - 581 °F
A. Schulman SCHULAMID® 66 MV3FR Flame Retardant Nylon 6/6
Information provided by A. Schulman.
Melt Temperature 280 - 305 °C
536 - 581 °F
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6
Information provided by A. Schulman.
Melt Temperature 280 - 305 °C
536 - 581 °F
A. Schulman SCHULAMID® 66 MV3HI High Impact Nylon 6/6
Information provided by A. Schulman.
Melt Temperature 295 - 305 °C
563 - 581 °F
A. Schulman SCHULAMID® 66 MK40HI 40% Mineral Reinforced, Impact Modified 66
Information provided by A. Schulman.
Melt Temperature 280 - 305 °C
536 - 581 °F
A. Schulman SCHULAMID® 66 MV3FR Flame Retardant Nylon 6/6
Information provided by A. Schulman.
Melt Temperature 280 - 305 °C
536 - 581 °F
A. Schulman SCHULAMID® E-17222 High Impact Nylon 66
Information provided by A. Schulman.
Melt Temperature 295 - 305 °C
563 - 581 °F
A. Schulman SCHULAMID® 66 MK20HI 20% Mineral Reinforced, Impact Modified Nylon 66
Information provided by A. Schulman.
Melt Temperature 290 - 305 °C
554 - 581 °F
Covestro Makrolon® AL 2647 Polycarbonate, Automotive Lens Injection Grade
Easy flowing injection molding grade, UV-stabilized, easy mold release agent.Applications: Automotive lens applications, fulfills U.S. specification SAE J 576C.Information provided by Bayer.As of 1 ..
Melt Temperature 260 - 305 °C
500 - 581 °F
Extrusion Coating
DuPont™ Appeel® 45D747 Polyolefin
Appeel® 45D747 is a modified polyolefin resin designed to provide easy peel functionality from polyethylene copolymers. Appeel® 45D747 is available in pellet form for use in conventional extrusion..
Melt Temperature 285 - 305 °C
545 - 581 °F
DAM
DuPont Performance Polymers Minlon® EFE6096 GY090A Nylon 66  (Unverified Data**)
Minlon® EFE6096 GY090A is a 15% mineral reinforced impact modified nylon 66 resin.Information provided by DuPont Performance Polymers
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
Melt Temperature 280 - 305 °C
536 - 581 °F
BASF Ultramid® 82335G HS BK 102 50% Glass Filled PA6 (Conditioned)
Description: Ultramid 8235G HS BK-102 is a heat stabilized, pigmented black, 50% glass fiber reinforced PA6 injection molding compound offering excellent level of strength, stiffness, high temperatu..
Melt Temperature 280 - 305 °C
536 - 581 °F
BASF Ultramid® 82335G HS BK 102 50% Glass Filled PA6 (Dry)
Description: Ultramid 8235G HS BK-102 is a heat stabilized, pigmented black, 50% glass fiber reinforced PA6 injection molding compound offering excellent level of strength, stiffness, high temperatu..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R535H NT651 Nylon 66, 35% Glass Reinforced, DAM
Vydyne® R535H NT651 is 35% glass-fiber reinforced PA66 resin. Available in natural, it is heat-stabilized with an electrically neutral heat stabilizer. It is designed specially for electrical appli..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. ..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G..
Melt Temperature 280 - 305 °C
536 - 581 °F
BASF Ultramid® HMG14 HS BK 102 60% Glass Filled PA66 (Dry)
Description: Ultramid HMG14 HS BK-102 is a 60% glass reinforced, injection molding grade of PA66 offering high strength and stiffness. Due to inherently lower moisture absorption, Ultramid HMG14 HS ..
Melt Temperature 285 - 305 °C
545 - 581 °F
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra..
Melt Temperature 275 - 305 °C
527 - 581 °F
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded
Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb..
Melt Temperature 275 - 305 °C
527 - 581 °F
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded
Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com..
Melt Temperature 260 - 305 °C
500 - 581 °F
DuPont Nucrel® 0910HS-SR Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating  (discontinued **)<
8.7 wt% Methacrylic Acid.Nucrel® 0910HS-SR is an ethylene-methacrylic acid copolymer resin available for use in conventional and coextrusion coating equipment designed to process polyethylene resin..