Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Plastcom SLOVAMID 6 GB 30 PA6, 30% glass beads FeaturesNearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properti.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Plastcom SLOVAMID 6 GF 25 FRG 5 PA6, 25% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Plastcom SLOVAMID 6 GF 35 FRC 5 PA6 reinforced with 35% glass fibre, with flame retardant PA 6 for injection moulding, chemically reinforced with 35 % glass fibre, with halogen free flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 750°C, C.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Plastcom SLOVAMID 6 T 15 Polyamide 6, 15% Micronized Talc FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Plastcom SLOVAMID® 6 GF 30 FRG 2 PA6 reinforced with glass fiber, flame retarded PA 6 for injection molding, reinforced with 30 % glass fiber, flame retarded with halogen free flame retardant. Main features: flammability in accordance with UL 94 5 at 3.2 mm. Application for the .. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Plastcom SLOVAMID® 6 GF 40 HI PA6 reinforced with glass fiber, improved impact strength PA 6 for injection molding, reinforced with 40% glass fiber, impact modified. Application: impacted moldings and moldings with higher strength applied in automotive, electrical, engineering and cons.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Plastcom SLOVASTER® B GF 40 PBT reinforced with 40% glass fibre Features: PBT for injection moulding, chemically reinforced with 40% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Plastcom SLOVASTYR® B BT N PBT Regranulate PBT basic type for injection molding. Melt is characterized by very good fluidity, which enables injection molding of complicated and divided products also on multiple moulds. Anisotropy.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Plastcom SLOVAMID 6 GF 15 HI PA6, 15% glass fibre, improved strength FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Melt Temperature | 260 - 270 °C | 500 - 518 °F | Cast Film |
Honeywell Aegisâ„¢ H100ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100ZP is a medium viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well .. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Lanxess Pocan® B 5220 XF 000000 PBT, 20% Glass Spheres PBT, 20% glass spheres, injection molding, improved flowability, improved impact strength, low tendency to warpInformation provided by LANXESS. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
LATI Laticonther 82 CP1/800 PA12 High thermal conductivity product based on Polyamide 12 (PA12). Special fillerAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Melt Temperature | 240 - 270 °C | 464 - 518 °F | Injection Molding |
Styrolution Terblend® N NM-21 EF Gray 38058 ABS+PA (Conditioned) Description: Terblend® N NM-21 EF is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures. The enhanced flowability enables excellent processability and sur.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Sax Polymers SAXAMID 126H Nylon 6, Injection Molding Grade SAXAMID 126H is a general purpose polyamide 6 injection-molding-grade. Benefits are short cycle times and good release properties. Additionally it has a higher content of heat stabilizer which is p.. |
|||
Melt Temperature | 255 - 270 °C | 491 - 518 °F | |
Toyobo VYLOPET® EMC355 Injection Molding Polyester Resin, Glass Reinforced Applications: HousingsBracketsGear casesFeatures: High RigidityGlass fiber reinforcementInformation provided by Toyobo. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Eastman Drystar 0113 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Eastman Eastar DN001HF Copolyester Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN001HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Eastman Eastar MN004 Copolyester Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl.. |
|||
Melt Temperature | 220 - 270 °C | 428 - 518 °F | |
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Covestro Makroblend® DP UT3907 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT3907* offers superior flowability, good impact strength and excellent ch.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Covestro Makroblend® S 7916 Polycarbonate + PBT, Impact Grade ISO 7792-1-PBT/PC,MHPR,-020(PBT+PC)-blendsimpact modifiedInjection molding gradeexcellent chemical resistancehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessing.. |
|||
Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
Eurostar Staramide BG10HU PA6, 50% Glass Fiber Filled, UV and Heat Stabilized, Injection Molded Staramide BG10HU is an UV and Heat Stabilized, 50% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 230 - 270 °C | 446 - 518 °F | |
E-Polymers TEKASTER® F10G30 30% Glass Fiber Reinforced PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | Injection molding |
BASF Ultramid® S3K Balance PA 610 (Dry) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont.. |
|||
Melt Temperature | 210 - 270 °C | 410 - 518 °F | |
Suzhou Hipro Polymers Hiprolon® 211 ESNNHL P40 Nylon Hiprolon® 211ESNNHL P40 is a long chain polyamide compound from bio-renewable resource. It features low density, low water absorption, high dimension stability, high cold impact resistance, high bu.. |
|||
Melt Temperature | 250 - 270 °C | 482 - 518 °F | Injection molding/Extrusion |
BASF Ultradur® B 4300 G2 FC 10% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |