Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Polymer Resources PC-FD4-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Polymer Resources PC-GP4-[color]-4 Polycarbonate, UV-stabilized, Easy Flow with Mold Release Polycarbonate, UV-stabilized, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Melt Temperature | 266 - 282 °C | 511 - 540 °F | |
PolyOne Edgetek® X TR2-10GF/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Melt Temperature | 266 - 282 °C | 511 - 540 °F | |
PolyOne Edgetek® X TR2-10TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Melt Temperature | 266 - 282 °C | 511 - 540 °F | |
PolyOne Edgetek® X TR2-30TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Polymer Resources PC-UV4 Polycarbonate, UV-stabilized, Easy Flow Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
Ravago Manufacturing Americas Hylon® N1000STHLUV2 HF Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat Stabilized and High FlowRoHS CompliantAuto Specifications: GM GMP.PA66.074.. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax BFM40-DL04N1 Nylon 6 40% Mineral Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 282 °C | 510 - 540 °F | |
MRC Polymers NAXALOYâ„¢ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
MTI ThermoStran® PA66-40C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
MTI ThermoStran® PA66-60G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant 6604-HSL Nylon 66, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant PA131G2GN-91 Green Nylon 66, Highly Toughened Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol BRU0000BN-182 Nylon 66, Lubricated, Nucleated, Weather Resistant Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol PA101LRD-190 Nylon 66, General Purpose, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant Renol PCSP0006 Polycarbonate, Laser Markable Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol 6608 HSL Nylon 66, High Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol PA111G33 Nylon 66, 33% Glass Fiber Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 °C | 511 °F | |
Chem Polymer Chemlon 109 Nylon 66, High Impact A highly impact-modified, lubricated nylon 66 exhibiting excellent toughness, especially at lower temperatures.Data provided by the manufacturer, Chem Polymer. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG30-QN11N1 Nylon 6 30% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG30-SN31N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG30-SN31N1 Nylon 6 30% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG33-RN13N1 Nylon 6 33% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG35-R113N1 Nylon 6 36% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG45-RN13N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |