Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chem Polymer Chemlon 109 Nylon 66, High Impact

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Chem Polymer
Trade Name Chemlon
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Chemlon 109 Nylon 66, High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A highly impact-modified, lubricated nylon 66 exhibiting excellent toughness, especially at lower temperatures.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 49.0 MPa
7110 psi
ASTM D638
Elongation at Break 55 %
55 %
ASTM D638
Flexural Yield Strength 63.0 MPa
9140 psi
ASTM D790
Flexural Modulus 1.70 GPa
247 ksi
ASTM D790
Izod Impact, Notched 8.48 J/cm
15.9 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 252 °C
486 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Melt Temperature 266 °C
511 °F