Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gromax CFG33-RN13N1 Nylon 6 33% Glass Filled (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Gromax
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gromax CFG33-RN13N1 Nylon 6 33% Glass Filled (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Gromax Enterprises Corp.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ISO 1183
Moisture Absorption 0.860 %
0.860 %
ISO 62
Maximum Moisture Content 0.10
0.10
Karl Fischer
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 222 °C
432 °F
ISO 75-1,-2
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Processing Properties Metric English Comments
Melt Temperature 266 - 280 °C
511 - 536 °F
ISO 294
Mold Temperature 80.0 - 120 °C
176 - 248 °F
ISO 294
Drying Temperature 80.0 °C
176 °F
Dry Time 2.00 - 6.00 hour
2.00 - 6.00 hour