Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom PLASTALEN® PH 51 T 40 Polypropylene reinforced with mineral filler Modified homopolymer PP for injection molding with the content of 40% mineral filler. General application. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PC 18 FRT 5 PP, mod. of mech. properties, fire retardant FeaturesModified copolymer PP for extrusion, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Delivered in natural mode and in the full RAL colour sc.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PC 51 C 30 Polypropylene Homopolymer and Copolymer, 30% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 30% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C... |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PC 51 T 20 Polypropylene Copolymer, 20% Micronized Talc FeaturesModified copolymer PP for injection moulding with the content of 20% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden f.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PH 61 B 70 PP, 70% mineral filling FeaturesModified PP for injection moulding with the content of 70% of barium sulphate. Increased density. Decreased shrinkage.Used for production of vertical blind weights. Delivered in natural mode.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PQ 91T 5 PP, 5% mineral filling FeaturesModified PP for injection moulding with the content of 5 % mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Melt Temperature | 200 °C | 392 °F | |
NatureWorks® Ingeo™ 8052D Foam Grade Biopolymer Ingeo 8052D can be converted into an expanded foam sheet with use temperatures up to 77°F (25°C). This foam is lightweight, strong and suitable for packaging fresh meat and vegetables. In order to.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | |
Polykemi AB POLYelast TPE EC88R Thermoplastic Elastomer, PP/EPDM Information provided by Polykemi AB |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Premix Thermoplastics PRE-ELEC® PP 1385 PRE-ELEC PP 1385 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Melt Temperature | 200 - 260 °C | 392 - 500 °F | |
Premix Thermoplastics PRE-ELEC® PP 1398 Conductive Thermoplastic Compound PRE-ELEC® PP 1398 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PC 53 N Polypropylene Copolymer, UV Stabilization FeaturesModified copolymer PP for injection moulding, with the ability of modeling the melt flow rate within the interval 5 - 20 g/10 min. Can be used for simple small as well as for large complica.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PC 93 T 5 PP reinforced with 5% mineral filler Features: Modified PP for injection moulding with the content of 5% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches.Packa.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PH 49 GF 10 Polypropylene Homopolymer, 10% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Melt Temperature | 200 - 210 °C | 392 - 410 °F | Injection Molding |
DuPont Performance Polymers Delrin® 127UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 127UVE NC010 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information pro.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP2150 PP+GF15% Description: Injection Molding, PP+GF15%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP2200 PP+GF20% Description: Injection Molding, PP+GF20%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL HG3200SK2 PP+MF20%, High Gloss Description: Injection Molding, PP+MF20%, High GlossApplication: Electrical & Electronic PartsCAS: 9003-07-0 and 7727-43-7Information provided by LG Chemical |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL HI5205 PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3400 PP+MF40% Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3402 PP+MF40% Description: Injection Molding, PP+MF40%, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Melt Temperature | 200 - 240 °C | 392 - 464 °F | |
LATI Latene® EP 22UVH2 MX/25 PP Copolymer, Mineral Reinforced Polypropylene copolymer (PPc) based compound. UV stabilized. Improved thermal stabilization. Special mineral filler. Very good surface appearance. Good elongation.Availability: Africa & Middle East;.. |
|||
Melt Temperature | 200 - 240 °C | 392 - 464 °F | Flat film |
Styrolution Polystyrol 143 E GR 21 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Plates |
Styrolution Polystyrol 486 M GR 2 PS Description: Polystyrol 486 M is a normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H or Polys.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | |
Borealis Beta (ß)-PP™ BE60-7032 Grey Polypropylene Homopolymer for Pressure Pipes, Fittings and Sheets Beta(ß)-PP BE60-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer with fine grained ß-modification crystalline structure leading to excellent impact strength even at lo.. |
|||
Melt Temperature | 200 - 220 °C | 392 - 428 °F | |
Borealis BorSafe™ ME3420 MDPE Compound for Pressure Pipes BorSafe™ ME3420 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an .. |
|||
Melt Temperature | 200 °C | 392 °F | Injection Molding |
Covestro Texin® 990R Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Baye.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PH 51 T 20 Polypropylene Homopolymer, 20% Mineral Filled FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filler. Increased rigidity, strength and thermal use up to 130°C. Decreased shrinkage. General application .. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PQ 83 T 10 PP, 10% mineral filling FeaturesModified PP + EPDM for injection moulding with the content of 10% mineral filler. Increased rigidity, strength and thermal. Decreased shrinkage. Application in automotive, covers of car chas.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PH 51 T 10 Polypropylene Homopolymer, 10% Mineral Filled FeaturesModified homopolymer PP for injection moulding with the content of 10% mineral filler. Increased rigidity, strength and thermal use up to 120°C. Decreased shrinkage. General application .. |