| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | |
|
PolyOne LubriOne™ ATT-000/5T Black Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | |
|
PolyOne Versollan™ RU 2205-9 Thermoplastic Elastomer (TPE)
Versollan™ RU 2205-9 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa..
|
|||
| Melt Temperature | 180 - 210 °C | 356 - 410 °F | |
|
Premix Thermoplastics PRE-ELEC® TPE 1502 Conductive Thermoplastic Compound
PRE-ELEC® TPE 1502 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri..
|
|||
| Melt Temperature | 180 - 210 °C | 356 - 410 °F | |
|
Premix Thermoplastics PRE-ELEC® TPE 1503 Conductive Thermoplastic Compound
PRE-ELEC® TPE 1503 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri..
|
|||
| Melt Temperature | 200 - 210 °C | 392 - 410 °F | Injection Molding |
|
DuPont Performance Polymers Delrin® 300TE BK602 Acetal Homopolymer
(Unverified Data**)
Delrin® 300TE BK602 is a medium-high viscosity toughened acetal homopolymer for injection molding with extremely low VOC emissions.Information provided by DuPont Performance Polymers
|
|||
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | Stock |
|
PolyOne Lubri-Tech™ AT-000/08T Acetal - 8% PTFE
(discontinued **)
Data provided by PolyOne.
|
|||
| Melt Temperature | 180 - 210 °C | 356 - 410 °F | |
|
LATI LATAN 13 G/303 30% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)
(discontinued **)
Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea..
|
|||
| Melt Temperature | 185 - 210 °C | 365 - 410 °F | |
|
Premix Thermoplastics PRE-ELEC® 12-033
(discontinued **)
PRE-ELEC 12-033 is a conductive thermoplastic compound based on a polyacetal copolymer with 30% carbon fiber. PRE-ELEC 12-033 exhibits excellent mechanical properties and electrical conductivity. Te..
|
|||
| Melt Temperature | 180 - 210 °C | 356 - 410 °F | Extrusion Range |
|
MBA Polymers PP 2123 Post-consumer recycled polypropylene copolymer
Available in standard black.Information provided by MBA Polymers.
|
|||
| Melt Temperature | 180 - 210 °C | 356 - 410 °F | |
|
LATI Lastilac AR-V0E ABS, Flame Retardant
Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. Very good surface appearance.Av..
|
|||
| Melt Temperature | 180 - 210 °C | 356 - 410 °F | |
|
LATI Latiohm 73-09 PD01 G/20 POM, 20% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyoxymethylene (POM). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati ..
|
|||
| Melt Temperature | 160 - 210 °C | 320 - 410 °F | Injection Molding |
|
Stellarchem DIOSHY® GP-935-UB2 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
|
Teknor Apex Telcar® OBC 2581B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
|
Teknor Apex Telcar® OBC 4555A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
|
Teknor Apex Telcar® TL EF-6100 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
|
Teknor Apex Telcar® TL EF-6177B-UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
|
Teknor Apex Telcar® TL-1025-75 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
|
Teknor Apex Telcar® TL-1123 BLK 111 Thermoplastic Elastomer
Uses: General Purpose; Grommets; Weather Stripping Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 1..
|
|||
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
|
Teknor Apex Telcar® TL-1137 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
|
Teknor Apex Telcar® TL-1522A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
|
Teknor Apex Telcar® TL-2555F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
|
Teknor Apex Telcar® TL-3954-70 Thermoplastic Elastomer
Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire ..
|
|||
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
|
Teknor Apex Telcar® TL-4145A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | Processing Temperature |
|
Teknor Apex Telcar® TL-93-T0488D-70UJ BLACK Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Melt Temperature | 193 - 210 °C | 379 - 410 °F | Molding |
|
Lubrizol Estane® 2103-90AE Thermoplastic Polyurethane Elastomer
Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
|
|||
| Melt Temperature | 193 - 210 °C | 380 - 410 °F | Extrusion |
|
Total Lumicene® mPE M 3410 EP Metallocene Medium Density Film Resin
(Unverified Data**)
Polyethylene: Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityHigh StiffnessGood puncture resistanceGood tear strengthGood heat sealing p..
|
|||
| Melt Temperature | 188 - 210 °C | 370 - 410 °F | Stock |
|
PolyOne Lubri-Tech™ AT-000/15T-2S Copolymer Acetal - 15% PTFE, 2% Silicone Lubricated
(discontinued **)
Data provided by PolyOne.
|
|||