Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 190 °C | 374 °F | |
Multibase TPSiV® 4000-80A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Melt Temperature | 190 - 210 °C | 374 - 410 °F | |
Polykemi AB POLYabs V0X ABS, Flame Retardant Information provided by Polykemi AB |
|||
Melt Temperature | 190 - 210 °C | 374 - 410 °F | |
Premix Thermoplastics PRE-ELEC® ESD 5350 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5350 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
Melt Temperature | 190 - 210 °C | 374 - 410 °F | |
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injectio.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | |
Polykemi AB POLYabs F00 GF15 ABS, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Injection Molding |
Polimeri Europa Edistir RK Polystyrene
(discontinued **) UL94 V-0, flame retarded, high impact polystyrene. This grade is suitable for injection moulding. It combines high mechanical strength, heat resistance and good processability.
Designation: Thermopl.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 1531 High Heat Crystal Polystyrene
(discontinued **) High flow and high heat resistance, Excellent clarityApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optical p.. |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Melt Temperature | 190 - 200 °C | 374 - 392 °F | |
LG Chemical LUCEL FW-715C Friction and Wear Resistant POM, Polymeric Wear Additive, CaCo3 Filled, Low Warpage, Antistatic LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5400 High Impact Polystyrene High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova FX530 Impact Polystyrene Features: Excellent environmental stress crack resistanceExcellent Izod impact strengthUL Classification 94 HBBalanced physical propertiesApplications: ExtrusionThermoformingSelected injection moldi.. |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | |
LATI Lastilac AR G/17-V0E ABS, 17% Glass Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability.Availability: Afri.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Processing Temperature |
Teknor Apex Uniprene® UN-1069E2 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Processing Temperature |
Teknor Apex Uniprene® UN-2640S Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Processing Temperature |
Teknor Apex Uniprene® UN-7010-40D-NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Melt Temperature | 190 - 218 °C | 374 - 424 °F | blown film equipment |
DuPont Nucrel® 0903HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0903HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design.. |
|||
Melt Temperature | 190 °C | 374 °F | |
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Processing Temperature |
Teknor Apex Uniprene® UN-1141A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | pre-drying required |
Corbion Purac Blend C High Heat, Impact Modified Homopolymer PLA Heat resistance higher than typical PLA is achieved by addition of a nucleating agent and PDLA homopolymer. Increased impact is produced by addition of impact modifier to the base grade; a small am.. |
|||
Melt Temperature | 190 - 200 °C | 374 - 392 °F | |
Eurostar Starflam M10009AP PP, Flame Retardant, Injection Molding Starflam M10009AP is an Unfilled Flame Retardant high fluidity Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | Injection-molding |
BASF Ultraform® N2640 E4 POM Description: Is a POM + MBS, elastomer-modified injection-molding grade with high toughness and high weld line strength.Information provided by BASF |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Injection-molding |
BASF Ultraform® W2320 003 PRO POM Description: Is a POM, is a very easy flowing grade for thin-walled components with long flow paths.Information provided by BASF |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | Injection-molding |
BASF Ultraform® W2320 U035 LEV POM Description: Is a POM, UV-stabilized, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 4210 Medium Impact Polystyrene
(discontinued **) Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless o.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5460 High Impact Polystyrene
(discontinued **) High impact, Good environmental stress crack resistance, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on inject.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 204L Crystal Polystyrene General Purpose Grade
(discontinued **) Fast cycling, Good heat resistance, Good balance of properties and flow characteristics, Extrusion and Injection Molding Applications: General purpose injection molded itemsProperties were determin.. |