Processing Properties | Metric | English | Comments |
---|---|---|---|
Roll Temperature | 60.0 °C | 140 °F | 3rd Roll |
Premix Thermoplastics PRE-ELEC® ABS 1415 Conductive Thermoplastic Compound PRE-ELEC® ABS 1415 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® ABS.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® ESD 6010 Dissipative Masterbatch, IDP Additive PRE-ELEC® ESD 6010 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative pro.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® ESD 6020 Dissipative Masterbatch, IDP Additive PRE-ELEC® ESD 6020 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative pro.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 2nd Roll |
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® ESD 6600 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6000 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6000 has b.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 2nd Roll |
Premix Thermoplastics PRE-ELEC® ESD 6600 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6000 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6000 has b.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 2nd Roll |
Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has b.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 2nd Roll |
Premix Thermoplastics PRE-ELEC® ESD 7100 PRE-ELEC ESD 7100 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7100 has been developed for inject.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 2nd Roll |
Premix Thermoplastics PRE-ELEC® ESD 7200 PRE-ELEC ESD 7200 is a static dissipative thermoplastic compound based on PC/ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7200 has been developed for inj.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 2nd Roll |
Premix Thermoplastics PRE-ELEC® PE 1291 PRE-ELEC PE 1291 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 2nd Roll |
Premix Thermoplastics PRE-ELEC® PE 1294 PRE-ELEC PE 1294 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 2nd Roll |
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 2nd Roll |
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 3rd Roll |
Premix Thermoplastics PRE-ELEC® PP 1397 Conductive Thermoplastic Compound PRE-ELEC® PP 1397 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 3rd Roll |
Premix Thermoplastics PRE-ELEC® PS 1326 PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Roll Temperature | 60.0 °C | 140 °F | 3rd Roll |
Premix Thermoplastics PRE-ELEC® PS 1331 Carbon Black Filled Conductive Thermoplastic Compound PRE-ELEC® PS 1331 is a carbon black filled conductive thermoplastic compound based on polystyrene. In addition to a low electrical resistivity PRE-ELEC® PS 1331 has excellent mechanical properties.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 2nd Roll |
Premix Thermoplastics PRE-ELEC® TPE 1501 Conductive Thermoplastic Compound PRE-ELEC® TPE 1501 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 2nd Roll |
Premix Thermoplastics PRE-ELEC® TPE 1502 Conductive Thermoplastic Compound PRE-ELEC® TPE 1502 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 1st Roll |
Premix Thermoplastics PRE-ELEC® TPE 1503 Conductive Thermoplastic Compound PRE-ELEC® TPE 1503 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 2nd Roll |
Premix Thermoplastics PRE-ELEC® TPE 1503 Conductive Thermoplastic Compound PRE-ELEC® TPE 1503 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 2nd Roll |
Premix Thermoplastics PRE-ELEC® CP 1315
(discontinued **) PRE-ELEC CP 1315 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 3rd Roll |
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **) PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Roll Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Bottom, Extrusion |
LG Chemical LG713 ABS, Low Gloss Feature: Extrusion Molding, Low Gloss, ExtrusionApplication: Automotive Interior Housing (Cover Etc)CAS No. 25120-20-1, 9003-56-9 and 31621-07-5Information provided by LG Chemical |
|||
Roll Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Bottom |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Roll Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Bottom, Extrusion |
LG Chemical PI642G ABS, General Purpose, High Modulus Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Bottom, Extrusion |
LG Chemical RS650 ABS Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Bottom, Extrusion |
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Roll Temperature | 60.0 °C | 140 °F | 3rd |
Kostat E-2001 Conductive PP Compound KOSTAT E-2001 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using a special conductive carbon black. In addition to a low electrical resistivity, E-200.. |
|||
Roll Temperature | 60.0 °C | 140 °F | 3rd |
Kostat E-3007J Conductive PS Compound KOSTAT E-3007J is a conductive thermoplastic compound based on impact modified polystyrene and a special conductive carbon black.KOSTAT E-3007J is not dependant on atmospheric conditions.Special Fea.. |
|||
Roll Temperature | 60.0 - 90.0 °C | 140 - 194 °F | Bottom, Extrusion |
LG Chemical MA221 ABS, High Impact, Low Gloss Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |