Processing Properties Metric English Comments
Roll Temperature 60.0 °C
140 °F
3rd Roll
Premix Thermoplastics PRE-ELEC® ABS 1410
PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141..
Roll Temperature 60.0 °C
140 °F
1st Roll
Premix Thermoplastics PRE-ELEC® ESD 6020 Dissipative Masterbatch, IDP Additive
PRE-ELEC® ESD 6020 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative pro..
Roll Temperature 60.0 °C
140 °F
2nd Roll
Premix Thermoplastics PRE-ELEC® ESD 6020 Dissipative Masterbatch, IDP Additive
PRE-ELEC® ESD 6020 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative pro..
Roll Temperature 60.0 °C
140 °F
2nd Roll
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be..
Roll Temperature 60.0 °C
140 °F
1st Roll
Premix Thermoplastics PRE-ELEC® ESD 6600 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6000 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6000 has b..
Roll Temperature 60.0 °C
140 °F
2nd Roll
Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has b..
Roll Temperature 60.0 °C
140 °F
1st Roll
Premix Thermoplastics PRE-ELEC® ESD 7100
PRE-ELEC ESD 7100 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7100 has been developed for inject..
Roll Temperature 60.0 °C
140 °F
2nd Roll
Premix Thermoplastics PRE-ELEC® PE 1294
PRE-ELEC PE 1294 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129..
Roll Temperature 60.0 °C
140 °F
2nd Roll
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound
PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o..
Roll Temperature 60.0 °C
140 °F
2nd Roll
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound
PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE..
Roll Temperature 60.0 °C
140 °F
3rd Roll
Premix Thermoplastics PRE-ELEC® PET 1451
PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14..
Roll Temperature 60.0 °C
140 °F
3rd Roll
Premix Thermoplastics PRE-ELEC® PP 1386
PRE-ELEC PP 1386 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
Roll Temperature 60.0 °C
140 °F
3rd Roll
Premix Thermoplastics PRE-ELEC® PP 1391 Conductive Thermoplastic Compound
PRE-ELEC® PP 1391 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Roll Temperature 60.0 °C
140 °F
3rd Roll
Premix Thermoplastics PRE-ELEC® PP 1393 Conductive Thermoplastic Compound
PRE-ELEC® PP 1393 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity,..
Roll Temperature 60.0 °C
140 °F
3rd Roll
Premix Thermoplastics PRE-ELEC® PP 1397 Conductive Thermoplastic Compound
PRE-ELEC® PP 1397 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Roll Temperature 60.0 °C
140 °F
3rd Roll
Premix Thermoplastics PRE-ELEC® PS 1326
PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
Roll Temperature 60.0 °C
140 °F
3rd Roll
Premix Thermoplastics PRE-ELEC® PS 1331 Carbon Black Filled Conductive Thermoplastic Compound
PRE-ELEC® PS 1331 is a carbon black filled conductive thermoplastic compound based on polystyrene. In addition to a low electrical resistivity PRE-ELEC® PS 1331 has excellent mechanical properties..
Roll Temperature 60.0 °C
140 °F
1st Roll
Premix Thermoplastics PRE-ELEC® TPE 1503 Conductive Thermoplastic Compound
PRE-ELEC® TPE 1503 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri..
Roll Temperature 60.0 °C
140 °F
2nd Roll
Premix Thermoplastics PRE-ELEC® CP 1316  (discontinued **)
PRE-ELEC CP 1316 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resis..
Roll Temperature 60.0 °C
140 °F
3rd Roll
Premix Thermoplastics PRE-ELEC® CP 1318  (discontinued **)
PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit..
Roll Temperature 60.0 - 90.0 °C
140 - 194 °F
Bottom, Extrusion
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow
Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information ..
Roll Temperature 60.0 - 90.0 °C
140 - 194 °F
Bottom, Extrusion
LG Chemical LG713 ABS, Low Gloss
Feature: Extrusion Molding, Low Gloss, ExtrusionApplication: Automotive Interior Housing (Cover Etc)CAS No. 25120-20-1, 9003-56-9 and 31621-07-5Information provided by LG Chemical
Roll Temperature 60.0 - 90.0 °C
140 - 194 °F
Bottom, Extrusion
LG Chemical MA210 ABS, Low Gloss
Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
Roll Temperature 60.0 - 90.0 °C
140 - 194 °F
Bottom, Extrusion
LG Chemical MU620 ABS, Low Deformation
Feature: Extrusion Molding, Low DeformationApplication: Mock-UpCAS No. 9003-56-9Information provided by LG Chemical
Roll Temperature 60.0 - 90.0 °C
140 - 194 °F
Bottom, Extrusion
LG Chemical PI641 ABS, High Impact
Feature: Extrusion Molding, General Purpose, High ImpactApplication: Pipe FittingCAS No. 9003-56-9Information provided by LG Chemical
Roll Temperature 60.0 - 90.0 °C
140 - 194 °F
Bottom, Extrusion
LG Chemical PI642G ABS, General Purpose, High Modulus
Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical
Roll Temperature 60.0 - 90.0 °C
140 - 194 °F
Bottom, Extrusion
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane
Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Roll Temperature 60.0 - 90.0 °C
140 - 194 °F
Bottom, Extrusion
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity
Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Roll Temperature 60.0 - 90.0 °C
140 - 194 °F
Bottom, Extrusion
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC
Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Roll Temperature 60.0 - 100 °C
140 - 212 °F
Average value: 80.7 °C Grade Count:5
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..
Copyright © lookpolymers.com All Rights Reserved