Processing Properties | Metric | English | Comments |
---|---|---|---|
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Versaflex™ CL2242 Thermoplastic Elastomer (TPE) Versaflex™ CL2242 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Versollan™ OM 1262NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-9 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Excellent Grip with Matte, Rubbery Finish - P.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PTS PCA-FR Eco-Friendly, High Flow, Flame Retardant PC/ABS Alloy This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Dynaflex™ G2701-1000-02 Thermoplastic Elastomer (TPE) Dynaflex™ G2701-1000-02 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Adhesion to Polypropylene - Excellent Colorability - Good .. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Dynaflex™ G2712-1000-02 Thermoplastic Elastomer (TPE) Dynaflex™ G2712-1000-02 is an easy processing TPE designed for injection molding and extrusion aplications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - High.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Dynaflex™ G2755-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2755-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypro.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - .. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Dynaflex™ G7930-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7930-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To.. |
|||
Screw Speed | 25 - 100 rpm | 25 - 100 rpm | |
PolyOne Dynaflex™ G7940-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Screw Speed | 25 - 100 rpm | 25 - 100 rpm | |
PolyOne Dynaflex™ G7940-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7940-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Screw Speed | 25 - 100 rpm | 25 - 100 rpm | |
PolyOne Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7950-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Termopol Termoton® K2GA3060A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Termopol Termoton® V2GA1050d TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
PolyOne Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2711-1000-00 is an easy process compound designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - O.. |
|||
Screw Speed | 25 - 100 rpm | 25 - 100 rpm | |
PolyOne Dynaflex™ G7640-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe.. |
|||
Screw Speed | 25 - 100 rpm | 25 - 100 rpm | |
PolyOne Dynaflex™ G7702-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7702-9001-02 is a performance TPE designed for a wide variety of applications. - Excellent Dimensional Stability - Excellent Heat Stability - High Resilience - Low Compression Set - Over.. |
|||
Screw Speed | 25 - 100 rpm | 25 - 100 rpm | |
PolyOne Dynalloy™ OBC 8100-N50 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N50 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics ABSFR2 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics ABSGF10 Molding Grade ABS With 10% Glass Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics ABSGF30 Molding Grade ABS With 30% Glass Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics ABSHFL Molding Grade ABS High Flow Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics ABSLG3030 Molding Grade ABS, Low Gloss Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics ABSLG5035 Molding Grade ABS, Low Gloss Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics PC/ABSFR9002 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics PC/ABSQX7004 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics PCGF10 Molding Grade PC with 10% Glass Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Star Plastics ABS3545 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Screw Speed | 25 - 100 rpm | 25 - 100 rpm | |
Advanced Polymer Alloys DuraGrip™ DGR 6060 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6060NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6060NC has an
excellent soft touch feel,.. |
|||
Screw Speed | 25 - 75 rpm | 25 - 75 rpm | |
Termopol Termoton® K2GA4055D TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |