| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled |
| Manufacturer | PolyOne Corporation |
| Trade Name | Bergadur™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Bergadur™ PB400 G30 H UF UV Polybutylene Terephthalate (PBT).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 85.0 MPa @Temperature 23.0 °C |
12300 psi @Temperature 73.4 °F |
ISO 527-2/5 |
| Elongation at Break | 1.6 % @Temperature 23.0 °C |
1.6 % @Temperature 73.4 °F |
ISO 527-2 |
| Tensile Modulus | 9.00 GPa @Temperature 23.0 °C |
1310 ksi @Temperature 73.4 °F |
ISO 527-2 |
| Charpy Impact Unnotched | 3.40 J/cm² @Temperature 23.0 °C |
16.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| Charpy Impact, Notched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 224 °C | 435 °F | |
| Flammability, UL94 | V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
UL 94 |
| Glow Wire Test | 960 °C | 1760 °F | Flammability Index; IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+15 ohm | 1.00e+15 ohm | IEC 60093 |
| Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 230 - 270 °C | 446 - 518 °F | |
| Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F | |
| Drying Temperature | 110 - 130 °C | 230 - 266 °F | |
| Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | UV Stabilizer | |
| Features | Flame Retardant | |
| Halogen Free | ||
| Filler / Reinforcement | Glass Fiber Reinforcement, 30% Filler by Weight | |
| Forms | Pellets | |
| Generic Material | PBT | |
| Generic Name | Polybutylene Terephthalate (PBT) | |
| Regional Availability | Europe |