Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 120 - 150 °C | 248 - 302 °F | Average value: 138 °C Grade Count:33 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Drying Temperature | 120 - 150 °C | 248 - 302 °F | Average value: 146 °C Grade Count:13 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Drying Temperature | 70.0 - 150 °C | 158 - 302 °F | Average value: 98.7 °C Grade Count:15 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Drying Temperature | 120 - 150 °C | 248 - 302 °F | Average value: 143 °C Grade Count:41 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Drying Temperature | 121 - 150 °C | 250 - 302 °F | Average value: 140 °C Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Drying Temperature | 121 - 150 °C | 250 - 302 °F | Average value: 142 °C Grade Count:30 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Drying Temperature | 50.0 - 150 °C | 122 - 302 °F | Average value: 122 °C Grade Count:15 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 GCE/600 PEEK, Glass/Mineral Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 50 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Larton GK/400 PPS, Glass/Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Carbon fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa &.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Larton G/40 I6 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Good elongation. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Laticonther 80 GCE/650 PPS, Glass/Mineral Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Glass fibers / Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Latilub 80-10T G/40 PPS, 40% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Latilub 80-40GRT PPS, Graphite/PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). Graphite / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Drying Temperature | 120 - 150 °C @Time 14400 sec |
248 - 302 °F @Time 4.00 hour |
|
Eurostar Starglas GX05052 PSU, Glass Fiber Filled Starglas GX05052 is a Glass Fiber Reinforced PSU resin (also known as Starglas PSU A 10V ¾)Information provided by Eurostar. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Latilub 80-15T G/30 PPS, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Latilub 80-17ST G/30 PPS, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). Silicone / PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Latilub 88/10-15T G/30 PEEK, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Latilub 88/10-15T K/30 PEEK, 30% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Latilub 88/10-10T Y/10 PEEK, 10% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Latilub 88/50-30GRT PEEK, Graphite/PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |