Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 140 °C @Time 7200 - 14400 sec |
284 °F @Time 2.00 - 4.00 hour |
Pre-drying in a dehumidifier |
Premix Thermoplastics PRE-ELEC® PBT 1455 PRE-ELEC PBT 1455 is a conductive thermoplastic compound based on PBT. Conductivity is achieved by using special conductive carbon black. PRE-ELEC PBT 1455 has excellent mechanical properties as wel.. |
|||
Drying Temperature | 140 °C @Time 10800 - 14400 sec |
284 °F @Time 3.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1500-0871 Polysulfone, with glass spheres Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Drying Temperature | 140 °C @Time 10800 - 14400 sec |
284 °F @Time 3.00 - 4.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1500-8299 Polysulfone, with PTFE, lubricant modified Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Drying Temperature | 140 °C | 284 °F | 3 hr. |
LG Chemical Lupox® PBT-GP-1000 High Flow PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 140 °C @Time 10800 sec |
284 °F @Time 3.00 hour |
|
LG Chemical Lupox® PBT-GP-1000 High Flow PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 140 °C | 284 °F | 3 hr. |
LG Chemical Lupox® PBT-GP-2150 15% GFR PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 140 °C @Time 10800 sec |
284 °F @Time 3.00 hour |
|
LG Chemical Lupox® PBT-GP-2150 15% GFR PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 140 °C @Time 10800 sec |
284 °F @Time 3.00 hour |
|
LG Chemical Lupox® PBT-GP-2156F 15% GFR Flame Retardant PBT General Purpose PBT, 15% Glass Fiber Reinforced, Weather Resistant, Flame Retardant, Non-Bleed. Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 140 °C | 284 °F | 3 hr. |
LG Chemical Lupox® PBT-GP-2300 30% GFR PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 140 °C | 284 °F | 3 hr. |
LG Chemical Lupox® PBT-GP-2306F 30% GFR Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 140 °C @Time 10800 sec |
284 °F @Time 3.00 hour |
|
LG Chemical Lupox® PBT-GP-2306F 30% GFR Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 140 °C | 284 °F | 3 hr. |
LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 140 °C @Time 10800 sec |
284 °F @Time 3.00 hour |
|
LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 140 °C | 284 °F | 3 hr. |
LG Chemical Lupox® PBT-HI1002FM Impact Modified, Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 140 °C | 284 °F | 3 hr. |
LG Chemical Lupox® PBT-LW5303F 30% Glass Filled Low Warp Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 140 °C @Time 10800 sec |
284 °F @Time 3.00 hour |
|
LG Chemical Lupox® PBT-LW5303F 30% Glass Filled Low Warp Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 140 - 180 °C @Time 10800 sec |
284 - 356 °F @Time 3.00 hour |
|
LATI Lapex A PES Polyether Sulfone (PES). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf.. |
|||
Drying Temperature | 140 - 180 °C @Time 10800 sec |
284 - 356 °F @Time 3.00 hour |
|
LATI Lapex R G/10 PPSU, 10% Glass Reinforced Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Drying Temperature | 140 - 180 °C @Time 10800 sec |
284 - 356 °F @Time 3.00 hour |
|
LATI Lapex R G/20 PPSU, 20% Glass Reinforced Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Drying Temperature | 140 °C | 284 °F | |
Toyobo VYLOPET® EMC605P PBT/PET Alloy, Anti-microbial Applications: Gas equipment partsFeatures: Good anti-microbialGood appearanceFlame resistantInformation provided by Toyobo. |
|||
Drying Temperature | 140 °C | 284 °F | |
Unitika P-1001A Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Drying Temperature | 140 °C | 284 °F | |
Unitika U-100 Engineering Plastic CAS No: 26590-50-1Information provided by Unitika Ltd. |
|||
Drying Temperature | 140 °C | 284 °F | |
Unitika UG-100-30 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Drying Temperature | 140 °C | 284 °F | |
E-Polymers SEPAZ® K140HF 40% Glass Fiber Reinforced Low Flash, High Flow PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |
|||
Drying Temperature | 140 °C | 284 °F | |
BASF Ultrason® E 2010 MR HP PESU Description: Unreinforced, medium viscosity standard injection molding grade for improved demolding behavior with Mold Release. PES-Blend with improved processibility. (High Productivity) Abbreviate.. |
|||
Drying Temperature | 140 °C | 284 °F | |
BASF Ultrason® E 2010 SW Q31 10088 PESU Information provided by BASF |
|||
Drying Temperature | 140 °C | 284 °F | |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
Drying Temperature | 140 °C | 284 °F | |
BASF Ultrason® S 3010 MR UN PSU Description: Unreinforced, higher viscosity injection molding and extrusion grade, tougher, with improved chemical resistance and demolding optimized. Abbreviated designation according to ISO 1043-1.. |
|||
Drying Temperature | 140 °C | 284 °F | |
E-Polymers SEPAZ® K130IM 30% Glass Fiber Reinforced Impact Modified PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |