Processing Properties Metric English Comments
Drying Temperature 140 - 150 °C
284 - 302 °F
PolyOne LubriOne™ SF-30GF/15T Polyphenylene Sulfide (PPS)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Drying Temperature 140 °C

@Time 7200 - 14400 sec
284 °F

@Time 2.00 - 4.00 hour
Pre-drying in a dehumidifier
Premix Thermoplastics PRE-ELEC® PBT 1455
PRE-ELEC PBT 1455 is a conductive thermoplastic compound based on PBT. Conductivity is achieved by using special conductive carbon black. PRE-ELEC PBT 1455 has excellent mechanical properties as wel..
Drying Temperature 140 °C

@Time 10800 - 14400 sec
284 °F

@Time 3.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1500-8299 Polysulfone, with PTFE, lubricant modified
Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca..
Drying Temperature 140 °C
284 °F
3 hr.
LG Chemical Lupox® PBT-GP-2150 15% GFR PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Drying Temperature 140 °C

@Time 10800 sec
284 °F

@Time 3.00 hour
LG Chemical Lupox® PBT-GP-2150 15% GFR PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Drying Temperature 140 °C

@Time 10800 sec
284 °F

@Time 3.00 hour
LG Chemical Lupox® PBT-GP-2300 30% GFR PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Drying Temperature 140 °C

@Time 10800 sec
284 °F

@Time 3.00 hour
LG Chemical Lupox® PBT-HI1002FM Impact Modified, Flame Retardant PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Drying Temperature 140 °C
284 °F
3 hr.
LG Chemical Lupox® PBT-LW5303 30% Glass Filled Low Warp PBT
Low Warpage. Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Drying Temperature 140 °C
284 °F
3 hr.
LG Chemical Lupox® PBT-LW5303F 30% Glass Filled Low Warp Flame Retardant PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Drying Temperature 140 - 180 °C

@Time 10800 sec
284 - 356 °F

@Time 3.00 hour
LATI Lapex R G/10 PPSU, 10% Glass Reinforced
Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Drying Temperature 140 - 180 °C

@Time 10800 sec
284 - 356 °F

@Time 3.00 hour
LATI Lapex R PPSU
Polyphenylene Sulfone (PPSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..
Drying Temperature 140 °C
284 °F
Teknor Apex Beetle® PET1610F Polyethylene Terephthalate, 50% Glass Fiber Reinforced
Notes: PET1610F is a 50% glass fiber reinforced grade of PET that offers good mechanical performance at elevated temperatures and excellent mold release. Processing Method: Injection Molding Forms: ..
Drying Temperature 140 °C
284 °F
Unitika L-1003PA
Heat resistance, creep resistance, and excellent lubricantInformation provided by Unitika Ltd.
Drying Temperature 140 °C
284 °F
Unitika P-1001 Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..
Drying Temperature 140 °C
284 °F
Unitika P-3001S Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..
Drying Temperature 140 °C
284 °F
Unitika P-5001 Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..
Drying Temperature 140 °C
284 °F
Unitika UG-100-20 Engineering Plastic
Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd.
Drying Temperature 140 °C
284 °F
Toyobo VYLOPET® EMC605P PBT/PET Alloy, Anti-microbial
Applications: Gas equipment partsFeatures: Good anti-microbialGood appearanceFlame resistantInformation provided by Toyobo.
Drying Temperature 140 °C
284 °F
Unitika P-1001A Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..
Drying Temperature 140 °C
284 °F
Unitika PT-3020
Characteristics: Dimensional accuracy (planarity) Heat resistance Creep resistance and elasticity RigidityInformation provided by Unitika Ltd.
Drying Temperature 140 °C
284 °F
Unitika UG-100-30 Engineering Plastic
Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd.
Drying Temperature 140 °C
284 °F
E-Polymers SEPAZ® K140HF 40% Glass Fiber Reinforced Low Flash, High Flow PPS Resin
Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit..
Drying Temperature 140 °C
284 °F
BASF Ultrason® E 2010 C6 30% Carbon Filled
Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu..
Drying Temperature 140 °C
284 °F
BASF Ultrason® P 3010 MR SW 10101 PPSU
Description: Unreinforced, higher viscosity injection molding grade, flame retardant and with improved chemical resistance. This grade is black colored and demolding optimized. Abbreviated designati..
Drying Temperature 140 °C
284 °F
BASF Ultrason® E 2010 HC PESU
Information provided by BASF
Drying Temperature 140 °C
284 °F
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE
Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, ..
Drying Temperature 140 °C
284 °F
Unitika P-3001 Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..
Drying Temperature 140 °C
284 °F
E-Polymers SEPAZ® K115HF 15% Glass Fiber Reinforced High Flow PPS Resin