| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled |
| Manufacturer | LG Chemical |
| Trade Name | Lupox® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | LG Chemical Lupox® PBT-GP-2150 15% GFR PBT.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.41 g/cc | 0.0509 lb/in³ | ASTM D792 |
| Water Absorption | 0.070 % | 0.070 % | 24 hours at 73°F; ASTM D570 |
| Linear Mold Shrinkage | 0.0040 - 0.011 cm/cm | 0.0040 - 0.011 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 90 | 90 | ASTM D785 |
| Tensile Strength, Ultimate | 93.1 MPa @Thickness 3.17 mm |
13500 psi @Thickness 0.125 in |
ASTM D638 |
| Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
| Elongation at Break | 4.0 % | 4.0 % | ASTM D638 |
| Flexural Yield Strength | 147 MPa | 21300 psi | ASTM D570 |
| Flexural Modulus | 4.90 GPa | 711 ksi | ASTM D570 |
| Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ASTM D648 |
| Flammability, UL94 | HB @Thickness 0.7937 mm |
HB @Thickness 0.03125 in |
UL94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 95 sec | 95 sec | ASTM D495 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 230 - 245 °C | 446 - 473 °F | |
| Middle Barrel Temperature | 235 - 250 °C | 455 - 482 °F | |
| Front Barrel Temperature | 240 - 250 °C | 464 - 482 °F | |
| Nozzle Temperature | 240 - 260 °C | 464 - 500 °F | |
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
| Mold Temperature | 50.0 - 100 °C | 122 - 212 °F | Surface |
| Drying Temperature | 120 °C | 248 °F | 5 hr. |
| 140 °C | 284 °F | 3 hr. | |
| 120 °C @Time 18000 sec |
248 °F @Time 5.00 hour |
||
| 140 °C @Time 10800 sec |
284 °F @Time 3.00 hour |
||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
| Shot Size | 40 - 80 % | 40 - 80 % | |
| Vent Depth | 0.00254 - 0.00381 cm | 0.00100 - 0.00150 in |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ram Speed Setting | Medium to Fast | |
| Screw Speed | Medium |