Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Polymer Resources NY66-FRG25 Flame Retardant Nylon 66, 25% Glass Reinforced Nylon 66, 25% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are.. |
|||
Rear Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Polymer Resources NY66-G13 Nylon 66, 13% Glass Reinforced Nylon 66, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Rear Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Polymer Resources NY66-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Rear Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Polymer Resources NY66-G43-[color]-H Nylon 66, 43% Glass Reinforced, Heat Stabilized Nylon 66, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Rear Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Polymer Resources NY66-IM2-G13-[color]-H Nylon 66, 13% Glass Reinforced, Impact Modified, Heat Stabilized Nylon 66, 13% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Rear Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Polymer Resources NY66-M40 Nylon 66, 40% Mineral Filled Nylon 66, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested.. |
|||
Rear Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Polymer Resources NY66-M40-[color]-H Nylon 66, 40% Mineral Filled, Heat Stabilized Nylon 66, 40% Mineral Filled, Lubricated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon .. |
|||
Rear Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC-FD3 Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Rear Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC-FD3-[color]-1 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Rear Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC-GP3-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, High Flow Polycarbonate, FDA-compliant Feedstocks, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Rear Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Ravago Manufacturing Americas Hylex® P1010LLT Polycarbonate Information provided by Ravago. |
|||
Rear Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Ravago Manufacturing Americas Hylex® P1310LLT Polycarbonate Information provided by Ravago |
|||
Rear Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled
(discontinued **) Information provided by MRC Polymers Inc. |
|||
Rear Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Polymer Resources NY66-G13-[color]-H Nylon 66, 13% Glass Reinforced, Heat Stabilized Nylon 66, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Rear Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Polymer Resources NY66-G43-[color]H Nylon, 43% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Rear Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Polymer Resources NY66-IM1-G13-[color]-H Nylon 66, 13% Glass Reinforced, Toughened and Heat Stabilized Nylon 66, 13% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Rear Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Polymer Resources NY66-IM1-G33 Nylon 66, 33% Glass Reinforced, Toughened Nylon 66, 33% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Rear Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Rear Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Firestone CG430-203 Nylon 6, 30% Fiberglass Filled Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone |
|||
Rear Barrel Temperature | 249 - 282 °C | 480 - 540 °F | |
LTL Color Compounds ColorFast® NY2115 Nylon 66 Super tough nylon 6,6 with excellent chemical resistance and ductilityAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
LTL Color Compounds ColorFast® PC150 Polycarbonate 15 melt high flow polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Rear Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
MRC Polymers NAXELLâ„¢ PC429HHI Polycarbonate, Impact Modified, High MFR, EZ Flow Good Property RetentionHeat and Dimensional StabilityHigh Melt Impact ModifiedMFR can be modified between 10 to 26 g/10minsCan be UV stabilizedGenerally for natural, colorable and can go blackIntern.. |
|||
Rear Barrel Temperature | 238 - 282 °C | 460 - 540 °F | |
Star Plastics PC/ABSQX7004 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Rear Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Samyang Trirex® PC-3025IR 10 MFI Clear Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 238 - 282 °C | 460 - 540 °F | |
Wellman Wellamid® 42LH XE-N Unfilled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc. |
|||
Rear Barrel Temperature | 238 - 282 °C | 460 - 540 °F | |
Wellman Wellamid® 42LH-N Unfilled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc. |
|||
Rear Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Wellman Wellamid® GS40-60 42LH-N 40% Glass Sphere Filled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Rear Barrel Temperature | 249 - 282 °C | 480 - 540 °F | |
Clariant 66G43HLS-Black Nylon 66, 43% Glass Fiber Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Rear Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Entec Hylex® P1010FR Polycarbonate Information provided by Ravago. |