Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Resinoid 1324 Phenolic Molding, Glass Reinforced

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Glass Filled
Manufacturer Resinoid
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resinoid 1324 Phenolic Molding, Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
ASTM D792A
Water Absorption <= 0.10 %
<= 0.10 %
24 hours R.T. ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Positive Mold; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 62.0 MPa
8990 psi
ASTM D651
Flexural Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 19.0 GPa
2760 ksi
ASTM D790
Compressive Strength 193 MPa
28000 psi
ASTM D695
Izod Impact, Notched 0.630 J/cm
1.18 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 11.6 kV/mm
295 kV/in
Short Time; Dry; ASTM D149
Arc Resistance 190 sec
190 sec
ASTM D495
Processing Properties Metric English Comments
Mold Temperature 155 - 180 °C
311 - 356 °F