Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Physical Properties Metric English Comments
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792A
Water Absorption 0.15 %
0.15 %
24 hours R.T. ASTM D570
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
Positive Mold; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 100
100
ASTM D785
Hardness, Rockwell M 120
120
ASTM D785
Tensile Strength, Ultimate 65.0 MPa
9430 psi
ASTM D651
Flexural Strength 166 MPa
24100 psi
ASTM D790
Flexural Modulus 17.0 GPa
2470 ksi
ASTM D790
Compressive Strength 276 MPa
40000 psi
ASTM D695
Izod Impact, Notched 0.473 J/cm
0.886 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
CTE, linear 38.0 µm/m-°C

@Temperature 20.0 °C
21.1 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 270 °C
518 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.20e+11 ohm-cm
1.20e+11 ohm-cm
ASTM D257
Dielectric Strength 14.6 kV/mm
371 kV/in
Short Time; Dry; ASTM D149
Arc Resistance 180 sec
180 sec
ASTM D495
Processing Properties Metric English Comments
Mold Temperature 155 - 180 °C
311 - 356 °F