Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)
(Unverified Data**) Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® 2011 Polyarylamide (PARA), 42% Mineral Filler
(discontinued **) Ixef 2011 is a general purpose, 42% mineral reinforcedpolyarylamide which exhibits high strength and stiffness, low warpage, and outstanding surface gloss.- Black: Ixef 2011/9000- Custom ColorableFe.. |
|||
Mold Temperature | 60.0 - 140 °C | 140 - 284 °F | Average value: 88.2 °C Grade Count:23 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-7277 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-7312/GN Polyamide 46, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-7330 Polyamide 46, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Highly dimensionally stable at elevated tem.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-7342 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-8250 Polyamide 46, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Highly dimensionally stable at elevated tem.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 46/CF/15 Polyamide 46, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Mold Temperature | 90.0 - 140 °C | 194 - 284 °F | for Mechanical and Structural Standard Molding |
Mitsui Arlen™ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Mold Temperature | 90.0 - 140 °C | 194 - 284 °F | for Electronic and Electric Standard Molding |
Mitsui Arlen™ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Mold Temperature | 90.0 - 140 °C | 194 - 284 °F | for Electronic and Electric Standard Molding |
Mitsui Arlen™ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Mold Temperature | 90.0 - 140 °C | 194 - 284 °F | for Mechanical and Structural Standard Molding |
Mitsui Arlen™ C230 30% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
LATI Larton GCE/600 PPS, Glass/Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
LATI Larton GK/400 PPS, Glass/Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Carbon fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa &.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
LATI Lasulf G/15 PSU, 15% Glass Fiber Reinforced Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort.. |
|||
Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
LATI Laticonther 80 CPG/700 PPS, Glass Fiber Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Special filler. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without s.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Teknor Apex Beetle® PET166F Polyethylene Terephthalate, 30% Glass Fiber Reinforced Notes: PET166F is a 30% glass fiber reinforced grade of PET that offers good mechanical performance at elevated temperature and excellent mold release. Processing Method: Injection Molding Forms: Pe.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Toyobo GLAMIDE® T-663G50A MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Covestro Apec® 1897 Polycarbonate Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=182 °CPreprocessingMax. Water content |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Eurotec® Tecopet® PT70 GR30 NL100 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Eurotec® Tecopet® PT74 GR30 BK002 DA PET, 30% glass fiber reinforced, high heat stabilized, black Information provided by Eurotec® |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA)
(Unverified Data**) Ixef 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 102.. |
|||
Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
LATI LARTON GCE/60 60% Mixed Glass Fiber and Special Mineral Filled Polyphenylene sulfide (PPS)
(discontinued Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Mold Temperature | 90.0 - 140 °C | 194 - 284 °F | for Electronic and Electric Standard Molding |
Mitsui Arlen™ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses .. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)
(discontinued **) Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope.. |
|||
Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
DuPont Performance Polymers Rynite® FG530 NC011 PET
(Unverified Data**) Rynite® FG530 NC011is a 30% glass fiber reinforced modified polyethylene terephthalate resin. It has been developed for consideration into applications for the food industry.Information provided by.. |