| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
|
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**)
Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15..
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
|
Solvay Specialty Polymers Ixef® 1023 Polyarylamide (PARA)
(discontinued **)
Ixef 1023 is a 50% glass-fiber reinforced, UV stabilized polyarylamide for interior applications, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resis..
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | Needed to develop high crystallinity |
|
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM
(discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
|
Lehmann & Voss LUVOCOM® 19-7276 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
|
Lehmann & Voss LUVOCOM® 19-7669 Polyamide 46, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot..
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
|
Lehmann & Voss LUVOCOM® 19-7827 Polyamide 46, with PTFE, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
|
Lehmann & Voss LUVOCOM® 19-7912 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.Gear parts f..
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
|
Lehmann & Voss LUVOCOM® 19-8365 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Mold Temperature | 80.0 - 140 °C | 176 - 284 °F | Start Point: 90°C |
|
Kingfa JH720 G30 30% Glass Fiber Reinforced PC
Features:High mechanical strengthGood size stabilityLow tendency to warpGood surfaceSuitable for exact moldingApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug parts..
|
|||
| Mold Temperature | 90.0 - 140 °C | 194 - 284 °F | for Electronic and Electric Standard Molding |
|
Mitsui Arlenâ„¢ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (COND)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
|
|||
| Mold Temperature | 90.0 - 140 °C | 194 - 284 °F | for Electronic and Electric Standard Molding |
|
Mitsui Arlenâ„¢ AE4200N Modified Nylon 6T, for Tribolic Applications, Flame Retardant (COND)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
|
|||
| Mold Temperature | 90.0 - 140 °C | 194 - 284 °F | for Mechanical and Structural Standard Molding |
|
Mitsui Arlenâ„¢ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (COND)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
|
|||
| Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
|
LATI Larton GCE/650 PPS, Glass/Mineral Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
|
|||
| Mold Temperature | 90.0 - 140 °C | 194 - 284 °F | for Electronic and Electric Standard Molding |
|
Mitsui Arlenâ„¢ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (DAM)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
|
|||
| Mold Temperature | 90.0 - 140 °C | 194 - 284 °F | for Mechanical and Structural Standard Molding |
|
Mitsui Arlenâ„¢ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (DAM)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
|
|||
| Mold Temperature | 130 - 140 °C | 266 - 284 °F | |
|
LATI Larton CE/60 PPS, 60% Mineral Reinforced
Polyphenylene Sulfide (PPS) based compound. Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; ..
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
|
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned)
Ixef® 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feature..
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
|
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA), 50% Glass Fiber
Ixef® 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance.Features: Flame Ret..
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
|
Solvay Specialty Polymers Ixef® FC-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned)
Ixef® FC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
|
Teknor Apex Beetle® PET1610F Polyethylene Terephthalate, 50% Glass Fiber Reinforced
Notes: PET1610F is a 50% glass fiber reinforced grade of PET that offers good mechanical performance at elevated temperatures and excellent mold release. Processing Method: Injection Molding Forms: ..
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
|
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro..
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
|
Covestro Apec® DP1-9354 Polycarbonate, Flame Retardant Grade
Developmental productflame retardant: V-0/1,5mm (UL 94)V-0/3,0mm (UL 94)5VA/3mm (UL 94)softening temperature (VST/B 120)=185 °Conly opaque colors availablePreprocessingMax. Water content
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
|
Eurotec® Tecopet® PT74 GR20 BK002 DA PET, 20% glass fiber reinforced, high heat stabilized, black
Information provided by Eurotec®
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
|
Eurotec® Tecopet® PT74 GR30 BK002 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black
Information provided by Eurotec®
|
|||
| Mold Temperature | 95.0 - 140 °C | 203 - 284 °F | |
|
Akro-Plastic Akromid® T6 GF 50 (3106) PPA Dry, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
|
|||
| Mold Temperature | 100 - 140 °C | 212 - 284 °F | Injection molding |
|
BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Conditioned)
Description: Ultramid® T 4381 LDS is a semi-crystalline, partially aromatic high temperature polyamide (PA6/6T) for laser direct structuring (LPKFLDS®). As the material is reinforced with 10% fibe..
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | Needed to develop high crystallinity |
|
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, at Equilibrium (65% RH)
(discontinu
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | Needed to develop high crystallinity |
|
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM
(discontinued **)<
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
|
|||
| Mold Temperature | 120 - 140 °C | 248 - 284 °F | Needed to develop high crystallinity |
|
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
|
|||
| Mold Temperature | 65.0 - 140 °C | 149 - 284 °F | Average value: 108 °C Grade Count:22 |
|
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..
|
|||