DuPont Performance Polymers Rynite® FG530 NC011 PET  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Rynite® FG530 NC011 PET  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Rynite® FG530 NC011is a 30% glass fiber reinforced modified polyethylene terephthalate resin. It has been developed for consideration into applications for the food industry.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Thickness 2.00 mm
0.0020 in/in

@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm

@Thickness 2.00 mm
0.0080 in/in

@Thickness 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 162 MPa

@Temperature 23.0 °C
23500 psi

@Temperature 73.4 °F
ISO 527
Elongation at Break 2.1 %

@Temperature 23.0 °C
2.1 %

@Temperature 73.4 °F
ISO 527
Tensile Modulus 10.5 GPa

@Temperature 23.0 °C
1520 ksi

@Temperature 73.4 °F
ISO 527
Charpy Impact Unnotched 4.00 J/cm²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 257 °C
495 °F
ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 242 °C
468 °F
ISO 75-1/-2
Processing Properties Metric English Comments
Melt Temperature 280 - 300 °C
536 - 572 °F
Mold Temperature 130 - 140 °C
266 - 284 °F
Drying Temperature 120 °C
248 °F
Dry Time 4.00 hour
4.00 hour
Moisture Content <= 0.020 %
<= 0.020 %
Descriptive Properties Value Comments
Appearance Natural Color
Forms Pellets
Generic PET
Material Status Preliminary Data
Part Marking Code >PET-GF30<
ISO 11469
Processing Method Injection Molding
Product Category Food Contact Resins
Glass Reinforced Resins
Region Available - Global Yes
Resin Identification PET-GF30
ISO 1043
RoHS Compliance Contact Manufacturer
Uses Food Applications, Non-specific