Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
Plastcom SLOVAMID 6 GF 15 T 25 LTS PA6, 15% glass fibre, 25% mineral filling FeaturesGood anisotropy of the manufacturing shrinkage. The talc is added to get the material shrinkage identical in both directions. Application for flat products in disc form /no screw after cooli.. |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
Polykemi AB POLYblend 45FS GK25 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
Polykemi AB POLYblend 85FS UV PC/ABS-Blend, UV stabilized Information provided by Polykemi AB |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | Average value: 81.7 °C Grade Count:3 |
Overview of materials for ABS/Polyester Alloy + GF This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro.. |
|||
Mold Temperature | 70.0 °C | 158 °F | DAM; optimum |
DuPont Performance Polymers Zytel® 103FHS BKB038 Nylon 66
(Unverified Data**) Zytel® 103FHS BKB038 is a heat stabilized, lubricated, PA 66 resin for fast cycling.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 70.0 - 120 °C | 158 - 248 °F | DAM |
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66
(Unverified Data**) Zytel® LM70G35HSLX is a 35% glass fiber reinforced, heat stabilized, lubricated polyamide 66 for injection molding. It is well suited for laser marking.Information provided by DuPont Performance Po.. |
|||
Mold Temperature | 70.0 - 110 °C | 158 - 230 °F | |
Lehmann & Voss LUVOCOM® 3-7451 Polyamide 6, lubricant modified, heat stabilized Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Mold Temperature | 70.0 - 110 °C | 158 - 230 °F | |
Lehmann & Voss LUVOCOM® 3-7723/ EG Polyamide 6, with carbon fiber, high viscosity Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressAntistatic.Handles, levers, rolle.. |
|||
Mold Temperature | 70.0 - 110 °C | 158 - 230 °F | |
Lehmann & Voss LUVOCOM® 6-7433 Polyamide 12, with carbon fiber, hydrolysis resistant Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Mold Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
LG Chemical IH830A PMMA, General Purpose Grade for Injection Molding Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and .. |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
LATI Latamid 66 H2 G/35-V0KB PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
LATI Kelon® B FR H CET/05-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
LATI Latamid SP1 PA 6.10 Polyamide 6.10 (PA6.10). Unfilled. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici .. |
|||
Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
LATI Latilub 73/13-01M POM, Molybdenum disulphide Filled Self-lubricating product based on Polyoxymethylene (POM). Molybdenum disulphide. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati In.. |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
Solvay TECHNYL® A 218C V10 PA66, 10% glass fiber, DRY Description: TECHNYL® A 218C V10 is a polyamide 66, reinforced with 10% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: Due to specially.. |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi.. |
|||
Mold Temperature | 70.0 - 160 °C | 158 - 320 °F | |
Solvay Specialty Polymers Xydar® MG-850 Liquid Crystal Polymer (LCP), 50% GlassMineral Xydar® MG-850 liquid crystal polymer (LCP) is a 50% glass/mineral reinforced injection molding grade developed for electrical/electronic applications utilizing surface mount technology. The mater.. |
|||
Mold Temperature | 70.0 °C | 158 °F | Injection Molding; ISO 294 |
Styrolution Novodur® P2M-V ABS Pellets Novodur® P2M-V has high impact strength, high gloss, and low emission. It is used for the production of molded plastic articles. |
|||
Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
Sax Polymers SAXAMID 136F3Q32 Nylon 6, 15% Glass Fiber SAXAMID 136F3Q32 is a high-impact-modified polyamide 6 injection-molding-grade reinforced with 15% glass fibers with very high impact properties. Beside the high impact strength at low temperatures .. |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
Topas Advanced Polymers TOPAS® IT X1 Cyclic Olefin Copolymer (COC) TOPAS® IT X1 is an injection molding grade with heat and impact resistance. It is a moderately clear resin with high moisture barrier, chemical and heat resistance, making it suitable for products .. |
|||
Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | actual surface temp |
Unitika UM-8430RG Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd. |
|||
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
CP-Polymer-Technik Wellamid® 6600 GV 25 HWCP 25% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
Eurostar Staramide ACF2 PA66, 10% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF2 is a 10% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
Eurostar Staramide AS10 PA66, 50% Glass Bead Reinforced, Injection Molding Staramide AS10 is a 50% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
Eurostar Starflam RFB247EX PA66/6, Glass Bead/Fiber Filled, Flame Retardant, Injection Molded RFB247EX is a Halogen Free and Red Phosphorous Free Flame Retardant, Glass Bead/ Glass Fiber Reinforced Polyamide 66/ Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 70.0 - 110 °C | 158 - 230 °F | |
Eurotec® Tecomid® NA40 GR20 NL HS PA6.6, 20% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Mold Temperature | 70.0 - 110 °C | 158 - 230 °F | |
Eurotec® Tecomid® NA40 GR30 NL IH PA6.6, 30% glass fiber reinforced, impact modified, natural Information provided by Eurotec® |
|||
Mold Temperature | 70.0 °C | 158 °F | Injection Molding; ISO 10724 |
Covestro Makroblend® DP UT3905 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseinjection molding grade Makroblend DP UT3905* offers superior flowability, good impact strength and excellent chemical resist.. |
|||
Mold Temperature | 70.0 - 120 °C | 158 - 248 °F | Average value: 93.3 °C Grade Count:34 |
Overview of materials for Acetal Copolymer + Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of .. |