| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Bead Filled |
| Manufacturer | Eurostar Engineering Plastics |
| Trade Name | Staramide |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Eurostar Staramide AS10 PA66, 50% Glass Bead Reinforced, Injection Molding.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
| Water Absorption at Saturation | 4.5 % @Temperature 23.0 °C |
4.5 % @Temperature 73.4 °F |
ISO 62-1 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | on Tensile Bar; E2P method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 85.0 MPa | 12300 psi | 5 mm/min; ISO 527 |
| Elongation at Break | 2.5 % | 2.5 % | 5 mm/min; ISO 527 |
| Tensile Modulus | 6.20 GPa | 899 ksi | 1 mm/min; ISO 527 |
| Flexural Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 6.00 GPa | 870 ksi | 2 mm/min; ISO 178 |
| Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -40.0 °C |
1.43 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
| 4.00 kJ/m² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A | |
| 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A | |
| Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | Edgew 80x10x4 sp=62; ISO 179/1eU |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
16.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
| CTE, linear, Transverse to Flow | 30.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
16.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
| Deflection Temperature at 1.8 MPa (264 psi) | 175 °C | 347 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Ae |
| Vicat Softening Point | 255 °C | 491 °F | B/120; ISO 306 |
| Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 400 V | 400 V | M; IEC 60112 |
| 500 V | 500 V | IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 1 | 260 - 280 °C | 500 - 536 °F | |
| Zone 2 | 260 - 280 °C | 500 - 536 °F | |
| Zone 3 | 270 - 290 °C | 518 - 554 °F | |
| Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
| Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
| Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
| Moisture Content | 0.20 % | 0.20 % |