Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 65.6 - 120 °C | 150 - 248 °F | Average value: 90.5 °C Grade Count:7 |
Overview of materials for Nylon 66, Mineral Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v.. |
|||
Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
Lehmann & Voss LUVOCOM® 1-7789/EG Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.High dimensi.. |
|||
Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
Lehmann & Voss LUVOCOM® 1-8070 VP Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Mold Temperature | 60.0 - 120 °C | 140 - 248 °F | |
Lehmann & Voss LUVOCOM® 1850-8322 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
Lehmann & Voss LUVOCOM® 21-8113 Polyamide 6/6T, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | |
Lehmann & Voss LUVOCOM® 50-7317 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | |
Lehmann & Voss LUVOCOM® 50-7844 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts; low thermal coefficient of expansion.Redu.. |
|||
Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | |
Lehmann & Voss LUVOCOM® 80/CF/12/TF/10/BK Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | |
Lehmann & Voss LUVOCOM® 80/TF/18/NT Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Mold Temperature | 40.0 - 120 °C | 104 - 248 °F | suitable temperature 60-80°C |
Gromax PBT 3030-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | |
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/HS-B Polyamide 66, with glass fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Heat stabilised.High dimension.. |
|||
Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
Lehmann & Voss LUVOCOM® 1/XCF/20 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
Lehmann & Voss LUVOCOM® 1-0866 Polyamide 66, with aramid reinforcement, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Improved heat resistance.Control disks, cams, sliding elements and other duty parts.. |
|||
Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
Lehmann & Voss LUVOCOM® G Polyamide 66, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Control disks, cams, sliding ele.. |
|||
Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | ISO 294 |
Gromax BTQ50-EQ00N1 Nylon 6, Impact Modified (Dry) Information provided by Gromax Enterprises Corp. |
|||
Mold Temperature | 100 - 120 °C | 212 - 248 °F | |
LATI Latilon 28D K/20 PC, 20% Carbon Fiber Reinforced Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b.. |
|||
Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | |
Solvay Specialty Polymers Kalix® 2930 HFFR Polyamide, High Performance (HPPA), Glass Fiber Kalix® 2930 HFFR is a bio-sourced polyamide-based material specifically formulated to meet UL 94V2 @ 0.4 mm requirements for electronic devices. The material uses an advanced halogen-free flame r.. |
|||
Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | |
Covestro Makrolon® 2558 Polycarbonate ISO 7391-PC,MR,(,,)-18-9MVR (300 °C/1.2 kg) 14.5 cm3/10 minMedical devicessuitable for ETO and steam sterilization at 121 °CComplies with the requirements of FDA-modified ISO 10993-1 and USP Class.. |
|||
Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
BASF Ultraform® E 3120 BM POM Description: Is a POM, high-molecular grade for extrusion blow molding of hollow parts.Information provided by BASF |
|||
Mold Temperature | 60.0 - 120 °C | 140 - 248 °F | Injection-molding |
BASF Ultraform® S2320 0035 LEV POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF |
|||
Mold Temperature | 60.0 - 120 °C | 140 - 248 °F | 80 - 90°C is recommended |
Azoty Tarnow™ Tarnamid® T-30 MS Polyamide 6 - Natural High viscosity extrusion grade for blown and flat films, including biaxial oriented films, also for extrusion of rods, pipes, plates, sheets, low diameter tubes and for injection molding of thick-wa.. |
|||
Mold Temperature | 21.1 - 120 °C | 70.0 - 248 °F | Average value: 73.5 °C Grade Count:8 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Mold Temperature | 40.0 - 120 °C | 104 - 248 °F | suitable temperature 60-80°C |
Gromax PBT 3015-104 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
Lehmann & Voss LUVOCOM® 1-7003 Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Mold Temperature | 70.0 - 120 °C | 158 - 248 °F | DAM |
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612
(Unverified Data**) Zytel® FE5382 BK276 is a 33% glass fiber reinforced, heat stabilized, black polyamide 612 resin developed for electrical bobbins and encapsulation applications.Information provided by DuPont Perfor.. |