Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 80.0 °C | 176 °F | |
NYCOA 2037 15% Glass Filled Nylon 6 15% glass filled very high viscosity nylon 6Information provided by NYCOA, Inc. |
|||
Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | |
Plastcom SLOVAMID 66 T 15 PA66, 15% mineral filling FeaturesPA 66 with the content of 15 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, automobile wheel.. |
|||
Mold Temperature | 80.0 °C | 176 °F | optimum |
DuPont Performance Polymers Crastin® SK605 BK851 PBT
(Unverified Data**) Crastin® SK605 BK851 is a 30% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
DuPont Performance Polymers Delrin® 100AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100AL NC010 an unreinforced, high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication for low wear and friction against metals and plastics.Informat.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
DuPont Performance Polymers Delrin® 311DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 311DP BK402 is a medium high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Informatio.. |
|||
Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | |
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS. |
|||
Mold Temperature | 80.0 °C | 176 °F | Injection Molding; ISO 10724 |
Lanxess Pocan® B 1700 000000 PBT PBT, non-reinforced, extrusion, food contact |
|||
Mold Temperature | 80.0 °C | 176 °F | Processing conditions for test specimens; ISO 294 |
Lanxess Pocan® B 3233 HR 000000 Polybutylene Terephthalate, 30% Glass Fibers PBT, 30% glass fibers, injection molding, improved flowability, hydrolysis stabilized |
|||
Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | ISO 294 |
Gromax BFG30-DN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | ISO 294 |
Gromax CFG45-RN13N1 Nylon 6 46% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
LATI Latamid 66 VH G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Hydrolysis stabilized. Glycol stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Solvay TECHNYL® A 218G1 V30 Black 34N PA66, 30% glass fiber, DRY Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. For 7.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Solvay TECHNYL® eXten D218 V30 Nylon 6.10, 30% glass fiber, DRY Description: TECHNYL® eXten D 218 V30 is a 30% Glass Fiber reinforced and heat stabilized product suitable to the manufacturing of all injection molded parts. This material is available in black... |
|||
Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | |
Solvay Specialty Polymers Kalix® 2855 Polyamide, High Performance (HPPA), Glass Fiber Kalix® 2855 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is formulated to provide maximum strength, stiffness, impact resistance, and p.. |
|||
Mold Temperature | 80.0 °C | 176 °F | ISO 294 |
Styrolution Terblend® N 3154 ASA / PA, 8% Mineral filled Terblend N 3154 is an 8% mineral filled ABS/PA blend with good dimensional stability and enhanced rigidity.High dimensional stabilityEnhanced rigidityMineral filled (8%)Information provided by Styro.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Toyobo GLAMIDE® TY-791HT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Mold Temperature | 80.0 °C | 176 °F | Injection molding; ISO 294 |
Covestro Makrolon® 2408 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Mold Temperature | 80.0 °C | 176 °F | Injection molding; ISO 294 |
Covestro Makrolon® FU4007 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
DuPont Performance Polymers Delrin® 300PE NC010A Acetal Homopolymer Delrin® 300PE NC010A is a medium-high viscosity acetal homopolymer, an enhanced version with extremely low VOC emissions. It has improved processing thermal stability, good mechanical properties, a.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Eurotec® Tecotek® PC43 GR003 TD70 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, light grey Information provided by Eurotec® |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Eurotec® Tecotek® PC43 GR20 BK002 PC, 20% glass fiber reinforced, black Information provided by Eurotec® |
|||
Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | Injection-molding |
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Dry) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Akro-Plastic Akromid® B3 (2500) PA 6 Dry AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Dry, 25% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Mold Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection Molding |
BASF Ultramid® B3WG6 GP BK 23210 30% Glass Filled PA6 (Conditioned) Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade used e.g. for automobile manifold.Information provided by BASF |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | |
LATI Latimass 62-01 D025 PA6 Specific density compound based on Polyamide 6 (PA6). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Mold Temperature | 80.0 °C | 176 °F | Injection Molding; ISO 10724 |
Lanxess Pocan® S 7020 000000 PBT PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified |
|||
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
LG Chemical LUMID LW4009A(W) PA6+GF/MF40%, Low Warpage Feature: Injection Molding, PA6+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |