Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products CS30P100-01UV 30% Ceramic Sphere Reinforced Polypropylene, UV Stabilized, Black Applications: Consumer goodsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products FT2700-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products FT3080-640UV Thermoplastic Polyolefin, UV Stabilized, BFQA Arizona Beige Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products FT4702-715UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey Applications: Exterior componentsGrillesBumper trimDoor componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products FT4802-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products FT4802-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bodyside moldings and claddingsFacia and bumper coversInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products FT4900-772UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products FT7016-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products GC45P200-01UV 45% Glass Fiber Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: BracketsUnderhood componentsLarge structural supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products GC8P200-00EG 8% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural, Extrusion Grade Applications: Extruded sheetWeather strippingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products HP514-489 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 101E Lite Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Interior trimIP structural componentsScuff/kick platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products P250-00 Polypropylene Copolymer, Natural Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products P252-00 Polypropylene Copolymer, Natural Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products P601-01 Polypropylene Copolymer, Black Applications: Engine componentChassis componentConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products RCC120-01 20% Calcium Carbonate Reinforced Polypropylene, Black, Recycled Content Applications: Electrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products T12P600-01BG 12% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade Applications: Flipper panelClose out panelSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 93.3 °C | 80.0 - 200 °F | |
Nilit Polynil® N66-P300 High Viscosity Nylon 6/6 Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 26.7 - 93.3 °C | 80.0 - 200 °F | |
PTS Trimid® N66-G13 13% Glass Fiber Reinforced Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products M15P101-01 15% Mica Reinforced Polypropylene, Black Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 54.4 °C | 80.0 - 130 °F | |
Styrolution Zylar 650 MBS Zylar® 650 is an impact modified styrene acrylic copolymer that provides a balance of clarity and toughness, with outstanding strength and rigidity. Zylar 650 also has superior processing charact.. |
|||
Mold Temperature | 26.7 - 60.0 °C | 80.0 - 140 °F | |
CTC SunPro® SP 200 P 3085 Polypropylene Copolymer SunPro® SP 200 P 3085 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: GM.PP... |
|||
Mold Temperature | 26.7 - 60.0 °C | 80.0 - 140 °F | |
CTC X-PRO CTC PP 4025 Polypropylene Copolymer X-PRO PP 4025 is a high value polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products CC20P200-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products GC20P255-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: BracketsUnderhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products GC30P104-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products CC20P100-00 20% Calcium Carbonate Reinforced Polypropylene, Natural Applications: ElectronicsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 26.7 - 48.9 °C | 80.0 - 120 °F | |
RheTech Products HP508-01UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trim, Close out panelsConsolesInjection molding conditions reported in table.Information provided by RheTech Products. |