Material Notes:
X-PRO PP 4025 is a high value polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
Physical Properties Metric English Comments
Melt Flow 15 g/10 min
15 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.2 MPa
2500 psi
ISO 527-1/2
Flexural Modulus 0.689 GPa
100 ksi
0.05 in/min; ISO 178
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ISO 180/A
Processing Properties Metric English Comments
Rear Barrel Temperature 182 - 216 °C
360 - 420 °F
Middle Barrel Temperature 193 - 227 °C
380 - 440 °F
Front Barrel Temperature 204 - 216 °C
400 - 420 °F
Nozzle Temperature 204 - 216 °C
400 - 420 °F
Melt Temperature 204 - 227 °C
400 - 440 °F
Mold Temperature 26.7 - 60.0 °C
80.0 - 140 °F
Back Pressure 0.345 - 1.03 MPa
50.0 - 150 psi
Clamp Pressure 27.6 - 34.5 MPa
4000 - 5000 psi
Descriptive Properties Value Comments
Boost Pressure (psi) 500-1500
Color General Purpose Black
Hold Pressure 50 - 75% of Boost
Screw Speed Medium to Fast