Polymer Property : Nozzle Temperature = 420 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 216 - 249 °C
420 - 480 °F
Multibase Multi-Pro® 2004 R Polypropylene
Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided ..
Nozzle Temperature 216 - 249 °C
420 - 480 °F
Multibase Multi-Pro® 3012 RC Polypropylene
Glass Fiber Reinforced, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products FT4650-583UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black
Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products FT4702-527UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic
Applications: Exterior door moldingsRigid bumper coversBodyside claddings and fairingsAutomotive grillesInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products FT4702-715UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey
Applications: Exterior componentsGrillesBumper trimDoor componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products FT4802-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Bodyside moldings and claddingsFacia and bumper coversInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products FT7011-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Claddings and faciasExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products GC20P100-177UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, (Chrysler HS5) Gray
Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products GC20P255-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Underhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products HP800-706UV 20% Talc Reinforced High Performance Polypropylene Copolymer, Scratch Resistant, UV Stabilized, Impact Modified, SWB White
Applications: Interior trim/Instrument panel componentsA/B pillarsGlove box doorsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products M20P100-01 20% Mica Reinforced Polypropylene, Black
Applications: Fan shroudsFiller panelsAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products M25P251-01A 25% Mica Reinforced Polypropylene Copolymer, Black
Applications: Fan shroudsInternal I/P componentsFiller panelsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products T20P100-517UV 20% Talc Reinforced Polypropylene, UV Stabilized, Interior DX9 Black
Applications: Center consolesIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products T20P250-00 20% Talc Reinforced Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products T20P250-01UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior componentsI/P componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products T20P250-699UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AC20157-120 Black
Applications: Window trimCowl screensExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products T20P252-00 20% Talc Reinforced Polypropylene, Natural
Applications: IP Structural componentsGlove box binWire troughInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products HP506-01A 21% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black
Applications: Automotive interior applicationsHVAC ductsTail lamp housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products HP531-01UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: IP structural componentsAir ducts - distributionA/B/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products HP534-00 22% Talc Reinforced High Performance Polypropylene Copolymer, Natural
Applications: Door trim panelsCenter consolesSteering columnsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products M25P251-01 25% Mica Reinforced Polypropylene Copolymer, Black
Applications: Fan shroudsGlove box binFiller panelsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 238 °C
420 - 460 °F
LTL Color Compounds ColorFast® ACR100IM Polymethylmethacrylate, High Impact
High impact version, extrusion or injection molding PMMAAll information provided by LTL Color Compounders, Inc.
Nozzle Temperature 216 - 249 °C
420 - 480 °F
LTL Color Compounds ColorFast® NYA1000 Nylon/ABS Alloy
Nylon/ABS alloy with high ductility and excellent chemical resistanceAll information provided by LTL Color Compounders, Inc.
Nozzle Temperature 216 - 249 °C
420 - 480 °F
LTL Color Compounds ColorFast® PBA2000 PBT/ABS Alloy, Flame Retarded
Flame-retarded V0-rated PBT/ABS alloyAll information provided by LTL Color Compounders, Inc.
Nozzle Temperature 216 - 238 °C
420 - 460 °F
MRC Polymers MAXTELâ„¢ 600T10-BK TPO, 10% Talc Filled
For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc.
Nozzle Temperature 216 - 238 °C
420 - 460 °F
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled
For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol..
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products CC20P200-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black
Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products CC20P100-00 20% Calcium Carbonate Reinforced Polypropylene, Natural
Applications: ElectronicsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 227 °C
420 - 440 °F
RheTech Products G20P100-406 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUEA) Midnight Black
Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Nozzle Temperature 216 - 232 °C
420 - 450 °F
Average value: 222 °C Grade Count:5
Overview of materials for Polypropylene with 30% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are..